The present invention relates to an ultralight foamed concrete wall composition including 90-98 wt% of a high early strength-type blended cement slurry, 1-8 wt% of waste foamed polystyrene having a density in a range of 0.002-0.010, a circular diameter, and a particle size of 2-15 mm, and 1-8 wt% of a foamed group obtained by diluting an animal or vegetable foaming agent in water at the ratio of 1:25-50 wt% and foaming using compressed air, and a manufacturing method of ultralight foamed concrete wall using the same. The high early strength-type blended cement slurry is obtained by mixing 50-80 wt% of a high early strength-type blended cement obtained by pulverizing 70-94 kg of a cement, 3-15 kg of calcium sulfoaluminate, 2-10 kg of anhydrous plaster and 1-5 kg of a slaked lime to a pulverized degree of 4,000-6,000 cm2/g, 20-50 wt% of water, and 0.1-0.5 wt% of a water reducing agent.
机译:本发明涉及一种超轻泡沫混凝土墙组合物,其包含90-98重量%的高早期强度型掺和水泥浆,1-8重量%的密度在0.002-0.010范围内的废泡沫聚苯乙烯,圆形通过将动物或植物发泡剂以1:25-50 wt%的比例稀释在水中并使用压缩空气发泡而获得的直径为2-15 mm的粒径,2-15 mm的粒径和1-8 wt%的发泡基团,以及使用其制造超轻泡沫混凝土墙的方法。通过混合50-80wt%的通过粉碎70-94kg的水泥,3-15kg的硫代铝酸钙,2-10kg的水泥而获得的高早强型混合水泥而获得高早强型混合水泥浆。将无水石膏和1-5千克熟石灰粉化至4,000-6,000 cm2 / g的粉碎度,20-50%的水和0.1-0.5%的减水剂。

著录项

  • 公开/公告号KR101406997B1

    专利类型

  • 公开/公告日2014-06-13

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20120104908

  • 申请日2012-09-21

  • 分类号C04B38/10;C04B28/16;C04B16/08;B28B1/50;

  • 国家 KR