SPRING STEEL WIRE ROD HAVING EXCELLENT WIRE DRAWABILITY AND EXCELLENT FATIGUE CHARACTERISTICS AFTER WIRE DRAWING, AND SPRING STEEL WIRE HAVING EXCELLENT FATIGUE CHARACTERISTICS AND EXCELLENT SPRING FORMABILITY

机译:拉伸后的弹簧钢丝具有出色的可焊性和优异的疲劳特性,而具有出色的疲劳特性和出色的弹簧可塑性的弹簧钢丝则具有出色的疲劳特性

摘要

This spring steel wire rod having excellent wire drawability and excellent fatigue characteristics after wire drawing and this spring steel wire having excellent fatigue characteristics and excellent spring formability are characterized by containing 0.50% or more but less than 0.70% of C, 1.0-2.5% of Si, 0.50-1.50% of Mn, 0.5% or less of Cr (including 0%), 0.001-0.005% of B, 0.005% or less of N (excluding 0%), 0.020% or less of P (excluding 0%), 0.020% or less of S (excluding 0%), 0.03% or less of Al (excluding 0%) and 0.0020% or less of O (excluding 0%), with the balance consisting of iron and unavoidable impurities, and are characterized in that the area ratio of the pearlite structure in the entire structure is 85% or more.
机译:该拉丝加工后的拉丝加工性,疲劳特性优异的弹簧钢丝以及疲劳特性和回弹加工性优异的弹簧钢丝的特征在于,含有0.50%以上且小于0.70%的C,1.0〜2.5%的C。 Si,Mn 0.50-1.50%,Cr 0.5%以下(含0%),B 0.001-0.005%,N 0.005%以下(N不包括0%),P 0.020%以下(不包括0%) ),S的0.020%以下(不包括0%),Al的0.03%以下(不包括0%)和O的0.003%以下(不包括0%),其余部分由铁和不可避免的杂质组成,并且其特征在于,珠光体组织在整个组织中的面积率为85%以上。

著录项

  • 公开/公告号KR101432464B1

    专利类型

  • 公开/公告日2014-08-20

    原文格式PDF

  • 申请/专利权人

    申请/专利号KR20137025442

  • 发明设计人 오우라 히로시;요시하라 나오;

    申请日2012-03-08

  • 分类号C22C38;F16F1/02;C21D8/06;C21D9/52;

  • 国家 KR

  • 入库时间 2022-08-21 15:40:16