1. A method of beneficiating slags containing high-grade steels and slags containing iron to extract metals, in which slags containing high-grade steels or slags containing iron are sent to the process of dry grinding, deagglomeration, classification and sorting and a metal fraction is formed and at least one silicate fraction, wherein the slags containing iron are preliminarily subjected to reduction treatment and fed as modified slags containing iron, while for grinding For grinding and deagglomeration, an abrasive mill with a runner path and grinding rolls rolling along the milled layer is used, while slag containing high-grade steels or modified slag containing iron are loaded into the abrasive mill with a grain size of the feed material of up to about 150 mm and grinding and deagglomeration are made depending on the type of slag, the metal content in the slag, the degree of adhesion and the required degree of purity of the metal and silicate fraction and the particle size of the finished product in the range of from 150 to 4,500 kN / m with respect to the vertically projected on the cup runners average diameter of the roll surface while maintaining the shape of metal chastits.2. The method according to claim 1, characterized in that a combination of an abrasive mill with a separator is used, in which grinding and deagglomeration are performed, and, if necessary, drying, as well as separation into a metal fraction and a silicate fraction. The method according to claim 2, characterized in that for grinding, deagglomeration, classification, sorting and drying,
机译:1.一种选矿方法,其中,将含有高等级钢的炉渣和含有铁的炉渣提取金属,其中,将含有高等级钢的炉渣或含有铁的炉渣送入干式粉碎,解团聚,分类选别以及金属分馏的工序。形成并形成至少一个硅酸盐馏分,其中含铁的炉渣预先进行还原处理,并作为含铁的改性炉渣进料,同时用于研磨和解团聚时,使用带有流道的研磨机和沿研磨机滚动的研磨辊使用高炉渣层时,将含高级钢的渣或含铁的改性渣装载到磨料磨机中,进料的粒度最大为约150毫米,并根据渣的类型进行研磨和解聚,炉渣中金属的含量,附着程度以及金属和硅酸盐级分所需的纯度以及f的粒径相对于垂直投射在辊道上的辊子表面平均直径为150至4,500 kN / m的成品,同时保持金属颗粒的形状.2。 2.根据权利要求1所述的方法,其特征在于,使用研磨机与分离器的组合,其中进行研磨和解聚,并且如果需要,进行干燥以及分离成金属级分和硅酸盐级分。 3.根据权利要求2所述的方法,其特征在于,对于研磨,解聚,分类,分选和干燥,

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号