1. A method for improving the uniformity of temperature in the heating furnace (200, 300), wherein the at least one heated bar (201, 301) obliquely leans against the inner wall of the heating furnace (200, 300) so that under the ingot (201, 301) between the ingot (201, 301) and the inner wall was a space (205, 305) of triangular cross section, wherein in a furnace supplied fuel, characterized in that at least one tube (230,240, 330, 340) for oxidant with an oxygen content of at least 85% by weight, is placed in the furnace wall so that it is inside the nozzle furnace (200, 300 ), And so that the oxidant can be fed directly into the said space (205, 305) at a rate of at least 100 m / c.2. A method according to claim 1, characterized in that the oxidant is supplied through a tube (330, 340), was reacted with the fuel in this space (305) under the ingot (301), wherein the fuel is supplied into the space (305) through a separate a tube (331, 341) for topliva.3. A method according to claim 1, characterized in that the major portion of the oxidant supplied through a tube (230, 240) is reacted with the CO formed during the fuel in the furnace of incomplete combustion (200) using an oxidant fed into the furnace, which It is not formed a space (205) under the ingot so that the furnace (200), combustion of fuel occurs in two etapa.4. A method according to claim 3, characterized in that the amount of oxidant fed to the furnace (200) is during combustion space (205) under the ingot is reduced so that the total fuel mixture in that part of the furnace, which has not formed a space (205) under ingot became substehiometricheskoy.5. A method according to any one of claims 1-4, characterized in that the oxidant is fed at least with a velocity zvuka.6. The method of
机译:1.一种用于提高加热炉(200、300)中的温度均匀性的方法,其中,至少一个加热棒(201、301)倾斜地倚靠在加热炉(200、300)的内壁上,从而锭(201、301)和内壁之间的锭(201、301)是具有三角形横截面的空间(205、305),其中在炉中供给燃料,其特征在于,至少一根管(230,240、330)氧含量至少为85%(重量)的氧化剂(340)放在炉壁内,使其位于喷嘴炉(200、300)的内部,从而可以将氧化剂直接送入所述空间(205,305)的速率至少为100 m / c.2。 2.根据权利要求1所述的方法,其特征在于,氧化剂通过管(330,340)供应,并与所述金属块(301)下方的该空间(305)中的燃料反应,其中,所述燃料被供应至所述空间(305)中。 305)穿过单独的topliva.3的管(331、341)。 2.根据权利要求1所述的方法,其特征在于,通过供给到炉中的氧化剂,使通过管(230、240)供应的氧化剂的大部分与在不完全燃烧炉(200)中的燃料期间形成的CO反应。 ,在铸锭下方未形成空间(205),因此炉(200)中的燃料燃烧发生在两个燃烧室中。4。 4.根据权利要求3所述的方法,其特征在于,减少了在所述铸块下方的燃烧空间(205)期间进给到所述炉子(200)的氧化剂的量,使得在尚未形成的炉子部分中的总燃料混合物锭子下面的空间(205)变成了substehiometricheskoy.5。 5.根据权利要求1-4中任一项所述的方法,其特征在于,所述氧化剂至少以速度zvuka.6进料。方法

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号