首页> 外国专利> Method of producing pig pipe size 289 × 11,5 × 26000-27000 AND 290 × 12 × × 26000-27500 mm TPU 8-16 'With pilger from ingots, electro-slag remelting BLANKS NIZKOPLASTICHNYH steels 04H14T3R1F-Sh-Sh 04H14T5R2F CONTAINING BORA 1.3 to 3.5 FOR MANUFACTURING PIPE hex-blank sizes 'turnkey' 257 + 2,0 / -3,0 × 6,0 + 2,0 / -1,0 × 4300 + 80 / - 30 mm for compact storage in the basin EXTRACTS AND TRANSPORTATION NPP spent nuclear fuel

Method of producing pig pipe size 289 × 11,5 × 26000-27000 AND 290 × 12 × × 26000-27500 mm TPU 8-16 'With pilger from ingots, electro-slag remelting BLANKS NIZKOPLASTICHNYH steels 04H14T3R1F-Sh-Sh 04H14T5R2F CONTAINING BORA 1.3 to 3.5 FOR MANUFACTURING PIPE hex-blank sizes 'turnkey' 257 + 2,0 / -3,0 × 6,0 + 2,0 / -1,0 × 4300 + 80 / - 30 mm for compact storage in the basin EXTRACTS AND TRANSPORTATION NPP spent nuclear fuel

机译:生产尺寸为289×11,5×26000-27000和290×12××26000-27500 mm TPU 8-16的生管的方法“用铸锭从皮尔斯,电渣重熔空白NIZKOPLASTICHNYH钢04H14T3R1F-Sh-Sh 04H14T5R2F含硼1.3至3.5%,用于制造管道六角尺寸“交钥匙” 257 + 2,0 / -3,0×6,0 + 2,0 / -1,0×4300 + 80 /-30 mm,用于紧凑型存放流域提取和运输NPP乏核燃料

摘要

FIELD: process engineering.;SUBSTANCE: invention relates to metallurgy, particularly to pipe production. Proposed process comprises production by ESR process of ingots sized to 500×1750±50 mm. Said ingots are turned to ingots-billets wised to 485±5×1750±50 mm, their weight making 2205-2440 kg. 100±5 mm diameter central bore is drilled therein. Ingots-billets in weight of 2106-2185 kg are grouped to one set. Ingots-billets in weight of 2190-2335 kg are grouped to another set. Said billets are heated to ductility temperature 1060-1090°C and pierced at helical rolling mill to get the sleeve billets Said sleeves are rolled to rerolled pipes at mandrels Carbon jar washer is fitted on said mandrel Said mandrel is fitted in the sleeve to produce the seed by rolling Sleeve with mandrel is returned to initial position to move the rolls together and to roll the front end.;EFFECT: preset sizes of rerolled pipes from ESR, higher efficiency of PRU 8-16" and decreased metal input.;3 cl, 1 tbl
机译:技术领域本发明涉及冶金学,尤其涉及管材生产。拟议的工艺包括通过ESR工艺生产尺寸为500×1750±50 mm的铸锭。将所述锭转变成明智的锭-坯料至485±5×1750±50mm,其重量为2205-2440kg。在其中钻出直径为100±5 mm的中心孔。重量为2106-2185千克的铸锭-方坯被分组为一组。重量为2190-2335千克的铸锭-方坯被分组为另一组。将所述坯料加热至延展温度1060至1090°C,并在螺旋轧机上刺穿以获得套筒坯料。将所述套筒在芯棒上轧制成再轧管。将碳罐垫圈安装在所述芯棒上。将所述芯棒安装在套筒上以生产芯棒。轧制种子,将带有心轴的套筒返回到初始位置,以使轧辊一起移动并轧制前端。;效果:通过ESR预设的轧制管尺寸,更高的PRU 8-16“效率和减少的金属输入。; 3厘升,1汤匙