首页> 外国专利> METHOD TO STRENGTHEN NATURAL SOILS AND MINERAL MATERIALS FOR CONSTRUCTION OF ROADS

METHOD TO STRENGTHEN NATURAL SOILS AND MINERAL MATERIALS FOR CONSTRUCTION OF ROADS

机译:加强道路施工的天然土壤和矿物材料的方法

摘要

FIELD: construction.;SUBSTANCE: in the method to strengthen natural soils and mineral materials for construction of roads with using of hydraulic mineral and water-dissolved polymer binders, including cement and latex of copolymers on the basis of sterol, ethers of acrylic acid, butadiene, acrylonitrile, ethylene with vinyl acetate, vinyl chloride or their mixtures with additives of thickeners on the basis of cellulose, defoaming agents of siloxane type and ether of glycol with regulation of pH by caustic, the specified polymer binder is used, polymer particles in which have dimensions from 50 to 200 nm, preferably 80-160 nm, with an additive in the amount of 0.1-5.0 wt parts per 100 wt parts of dry substance of the specified binder as a coalescer - ether of glycol of simple mono- or diester of ethylene- or diethylene glycol or aromatic hydrocarbon, for instance, white spirit, the value pH equal to 6.5-9 is set when using caustic in the form of 1-2% solution.;EFFECT: higher strength, water resistance.;10 ex, 4 dwg
机译:领域:建筑;物质:在使用水硬性矿物和水溶性聚合物粘合剂(包括基于固醇,丙烯酸醚的共聚物的胶乳和乳胶),水硬性矿物粘合剂和水溶性聚合物粘合剂来加固道路施工的天然土壤和矿物材料的方法中,丁二烯,丙烯腈,乙烯与乙酸乙烯酯,氯乙烯或它们与基于纤维素的增稠剂添加剂,硅氧烷型消泡剂和乙二醇醚(通过苛性碱调节pH值)的混合物,使用指定的聚合物粘合剂,聚合物颗粒其尺寸为50-200 nm,优选80-160 nm,且添加剂的量为每100重量份指定粘合剂干物质的0.1-5.0重量份,作为简单的单或二元醇的聚结剂-乙二醇醚乙二醇或二甘醇或芳族烃的二酯,例如石油溶剂油,当以1-2%溶液的形式使用苛性碱时,pH值等于6.5-9。耐性; 10 ex,4 dwg

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号