POLYESTER FIBER FOR ARTIFICIAL HAIR, MANUFACTURING METHOD THEREOF, FIBER BUNDLE FOR HAIR CONTAINING POLYESTER FIBER, AND HEAD DECORATION PRODUCT

机译:人造头发用聚酯纤维,其制造方法,含头发用聚酯纤维束和头部装饰产品

摘要

PROBLEM TO BE SOLVED: To provide a polyester fiber for artificial hair, a fiber having high fire retardancy and superior heat resistance, and a method of manufacturing the same, and to provide a fiber bundle for hair containing the same and a head decoration product.;SOLUTION: The polyester fiber for artificial hair of this invention contains a polyester resin and a brominated epoxy-based fire retardant. The polyester resin is a polyalkylene terephthalate and/or a copolyester comprising primarily a polyalkylene terephthalate, and intrinsic viscosity of the polyester resin is 0.3-0.5. A manufacturing method of the polyester fiber for artificial hair includes preferably a process of lowering the intrinsic viscosity of the polyester resin by a sugar alcohol-based and/or bisphenol-based compound which contains two or more hydroxyl groups in the molecule and which has a melting point of 80°C or higher and a boiling point of 260°C or higher.;COPYRIGHT: (C)2015,JPO&INPIT
机译:解决的问题:提供一种用于人造毛发的聚酯纤维,具有高阻燃性和优异的耐热性的纤维及其制造方法,并提供一种包含其的毛发纤维束和头部装饰产品。 ;解决方案:本发明的人造头发用聚酯纤维包含聚酯树脂和溴化环氧基阻燃剂。聚酯树脂是聚对苯二甲酸亚烷基酯和/或主要包含聚对苯二甲酸亚烷基酯的共聚酯,并且聚酯树脂的特性粘度为0.3-0.5。用于人造毛发的聚酯纤维的制造方法优选包括通过在分子中包含两个以上羟基的糖醇类和/或双酚类化合物降低聚酯树脂的特性粘度的步骤。熔点80°C或更高,沸点260°C或更高。;版权:(C)2015,日本特许经营&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号