A nickel recovery loss reduction method that makes it possible to reduce nickel recovery loss by lowering the concentration of fine floating solid components in overflow liquid in precipitating and separating treatments, and consequently to further reduce a nickel recovery loss, a hydrometallurgical method for nickel oxidized ore to which the nickel recovery loss reduction method is applied, and a sulfurizing treatment system. The present invention is a nickel recovery loss reduction method in a sulfurizing step for blowing hydrogen sulfide gas into a nickel containing sulfuric acid aqueous solution to generate nickel-containing sulfides and a barren liquid, and the nickel-containing sulfides with the average particle size adjusted to a predetermined size or larger are added as seed crystals to the sulfuric acid aqueous solution. It is more preferable to adjust the average particle size of the nickel sulfides to be added as seed crystals to 55 μm or more.
机译:一种通过降低沉淀和分离处理中溢流液中细微漂浮固体成分的浓度从而降低镍回收率的方法,从而进一步降低了镍回收率。一种用于镍氧化矿石的湿法冶金法应用镍回收减少损失法的方法,以及硫化处理系统。本发明是一种在硫化步骤中将镍的硫化氢气体吹入含镍的硫酸水溶液中以产生含镍的硫化物和贫瘠的液体的硫化步骤中镍回收损失减少的方法,并且调整了平均粒径的含镍的硫化物。将预定尺寸或更大尺寸的作为晶种加入到硫酸水溶液中。更优选将作为种晶而添加的硫化镍的平均粒径调整为55μm以上。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号