A method for preparing series of terpolymer of poly (diphenyl ether sulfone) and poly (diphenyl ether diphenyl sulfone) comprises: adding high temperature organic solvent, stirring and heating; sequentially adding 4,4′-dihydroxydiphenyl, 4,4′-dichlorodiphenyl sulfone and 4,4′-Bis(4-chlorophenyl)sulfonyl-1,1′-biphenyl; after all the monomers are completely dissolved, heating to 100° C. and adding alkali metal carbonate salt-forming agent which is 5-10 mol % more than the amount of 4,4′-dihydroxydiphenyl added, and subsequently adding xylene; continuously heating and salt-forming reaction begins in the system, and controlling the temperature at 190˜210° C.; then heating to 230˜236° C., and maintaining for 3-4 hours to obtain polymer viscous liquid; and refining the polymer viscous liquid to obtain a terpolymer containing different structural units in the molecular chain, wherein the Tg of the terpolymer can be regulated by changing the ratio of the two dichloro-containing monomers.
机译:一种聚二苯醚砜与聚二苯醚二苯砜系列三元共聚物的制备方法,包括:加入高温有机溶剂,搅拌并加热;依次加入4,4′-二羟基二苯基,4,4′-二氯二苯基砜和4,4′-双(4-氯苯基)磺酰基-1,1′-联苯;所有单体完全溶解后,加热至100℃,加入碱金属碳酸盐形成剂,该碱金属碳酸盐形成剂的量比4,4'-二羟基二苯基的加入量多5-10mol%,随后加入二甲苯;系统开始连续加热成盐反应,并将温度控制在190〜210℃。然后加热至230〜236℃,并保持3-4小时,得到聚合物粘稠液体。精制聚合物粘性液体,得到在分子链上含有不同结构单元的三元共聚物,其中三元共聚物的Tg可以通过改变两种含二氯单体的比例来调节。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号