(1) The total amount of the TiO2-equivalent content of the titanium compound, the Fe2O3-equivalent content of the iron compound and the alumina content is at least 98% by mass;(2) The total amount of the TiO2-equivalent content of the titanium compound and the Fe2O3-equivalent content of the iron compound is from 5 to 13% by mass."/> Method for producing alumina sintered body, alumina sintered body, abrasive grains, and grindstone
首页> 外国专利> Method for producing alumina sintered body, alumina sintered body, abrasive grains, and grindstone

Method for producing alumina sintered body, alumina sintered body, abrasive grains, and grindstone

机译:氧化铝烧结体的制造方法,氧化铝烧结体,磨粒和砂轮

摘要

Provided are a method for producing an alumina sintered compact satisfying the following (1) and (2), which comprises mixing and sintering an ilmenite powder and an alumina powder; the alumina sintered compact obtained according to the production method; and an abrasive grain and a grain stone.(1) The total amount of the TiO2-equivalent content of the titanium compound, the Fe2O3-equivalent content of the iron compound and the alumina content is at least 98% by mass;(2) The total amount of the TiO2-equivalent content of the titanium compound and the Fe2O3-equivalent content of the iron compound is from 5 to 13% by mass.
机译:提供一种满足以下(1)和(2)的氧化铝烧结体的制造方法,该方法包括将钛铁矿粉和氧化铝粉混合并烧结。根据生产方法获得的氧化铝烧结体;还有磨料和谷物。 (1)钛化合物Fe 2 O 3 的TiO 2 当量的总量-铁化合物和氧化铝的当量含量至少为98质量%; (2)TiO 的总量钛化合物的2 当量含量和铁化合物的Fe 2 O 3 当量含量为5〜13质量%。 ListItem>

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号