Provided is a heat-resistant cold rolled ferritic stainless steel sheet which contains, in terms of mass %, 0.02% or less of C, 0.1-1.0% of Si, greater than 0.6% to 1.5% of Mn, 0.01-0.05% of P, 0.0001-0.0100% of S, 13.0-20.0% of Cr, 0.1-3.0% of Mo, 0.005-0.20% of Ti, 0.3-1.0% of Nb, 0.0002-0.0050% of B, 0.005-0.50% of Al and 0.02% or less of N, with the remainder being Fe and unavoidable impurities, and which is characterized in that the areal proportion of grains having a {111} orientation in a region between a surface layer and a depth of t/4 (t is the sheet thickness) is 20% or higher, the areal proportion of grains having a {111} orientation in a region between a depth of t/4 and a depth of t/2 is 40% or higher, and the areal proportion of grains having a {011} orientation in the overall thickness region is 15% or lower.
机译:本发明提供一种耐热性冷轧铁素体系不锈钢板,其中,以质量%计,含有0.02%以下的C,0.1〜1.0%的Si,大于0.6%〜1.5%的Mn,0.01〜0.05%的Mn。 P,S 0.0001-0.0100%,Cr 13.0-20.0%,Mo 0.1-3.0%,Ti 0.005-0.20%,Nb 0.3-1.0%,B 0.0002-0.0050%,Al 0.005-0.50% N为0.02%以下,其余为Fe和不可避免的杂质,其特征在于,在表层与深度t / 4(t)之间的区域中,具有{111}取向的晶粒的面积比例。厚度为20%或更高时,在t / 4深度和t / 2深度之间的区域中具有{111}取向的晶粒的面积比为40%或更高,并且在整个厚度区域中具有{011}取向的晶粒为15%或更低。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号