process for the production of polypropylene varnish or paint of resin reinforced glicydylosiloksanowej trietylenotetraaminu0105 at elevated temperature by mixing resin glicydylosiloksanowej with trietylenotetraaminu0105 and ksylenem alternatively paste pigmentowu0105 features this,as a binder in the lacquer or paint is used glicydowosiloksanowu0105 resin of the formula (ch3) 3sio [si (ch3) 2o] m [si (ch3) {(ch2) 3och2choch2}] nsi (ch3) 3 in which m = 20 - 110, and n = 5 - 125 trietylenotetraaminu0105 composition in parts by weight: 85 - 95 resin glicydylosiloksanowej, 15 - 5 trietylenotetraam the other, with the curing varnish or paint is performed in the temp. 135 - 140u00b0c and 20 - 40 minutes.
机译:树脂cycydylosiloksanowej三苯甲基四氨基甲酸酯 u0105和ksylenem的混合,用于在高温下生产聚丙烯清漆或树脂增强的glicydylosiloksanowej trietylenotetraamin u0105的方法,或者粘贴颜料ow u0105的特点,因为在漆料或涂料中使用的粘合剂 glicydow0分子式为(ch3)3sio [si(ch3)2o] m [si(ch3){(ch2)3och2choch2}] nsi(ch3)3的树脂,其中m = 20-110,n = 5-125三乙烯四胺 u0105重量份组成:85-95树脂glicydylosiloksanowej,15-5三乙烯四胺,另一种是在临时用清漆或油漆进行的。 135-140 u00b0c和20-40分钟。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号