HIGH-STRENGTH CORROSION-RESISTANT TUBING FOR OIL AND GAS COMPLETION AND DRILLING APPLICATIONS, AND PROCESS FOR MANUFACTURING THEREOF

机译:高强度耐蚀管在油气完井和钻井应用中的应用及其制造工艺

摘要

A high strength corrosion resistant tubing comprises about 35 to about 55% Ni, about 12 to about 25% Cr, about 0.5 to about 5% Mo, up to about 3% Cu, about 2.1 to about 4.5% Nb, about 0.5 to about 3% Ti, about 0.05 to about 1.0% Al, about 0.005 to about 0.04% C, balance Fe plus incidental impurities and deoxidizers. The composition also satisfies the equation: (Nb−7.75 C)/(Al+Ti)=about 0.5 to about 9. A process for manufacturing the tubing includes: extruding the alloy to form a tubing; cold working the extruded tubing; annealing the cold worked tubing; and applying at least one age hardening step to the annealed tubing. Another process includes extruding the alloy at a temperature of about 2050° F. or less; annealing the extruded tubing; and applying at least one age hardening step to the annealed tubing.
机译:高强度耐腐蚀管包括约35至约55%的Ni,约12至约25%的Cr,约0.5至约5%的Mo,高达约3%的Cu,约2.1至约4.5%的Nb,约0.5至约5%。 3%的Ti,约0.05%至约1.0%的Al,约0.005%至约0.04%的C,余量的Fe以及附带的杂质和脱氧剂。该组成还满足等式:(Nb-7.75 C)/(Al + Ti)=约0.5至约9。一种制造管的方法包括:挤压合金以形成管;以及将合金挤出以形成管。对挤出管进行冷加工;对冷加工管进行退火;并将至少一个时效硬化步骤应用于退火管。另一种方法包括在约2050°F或更低的温度下挤出合金;然后将其挤出。对挤出管进行退火;并将至少一个时效硬化步骤应用于退火管。

著录项

  • 公开/公告号EP2734655A4

    专利类型

  • 公开/公告日2015-04-22

    原文格式PDF

  • 申请/专利权人 HUNTINGTON ALLOYS CORPORATION;

    申请/专利号EP20130804541

  • 发明设计人 MANNAN SARWAN KUMAR;

    申请日2013-04-12

  • 分类号C22C38;C21D1;C22C19/05;C22C38/44;C22F1/10;

  • 国家 EP

  • 入库时间 2022-08-21 15:05:51