METHOD FOR PRODUCING A COLD-ROLLED FLAT STEEL PRODUCT WITH HIGH YIELD STRENGTH AND FLAT COLD-ROLLED STEEL PRODUCT

机译:高屈服强度的冷轧平板钢材的生产方法和冷轧平板钢材的生产

摘要

The invention provides a method for producing a cold-rolled steel strip with a yield ratio Re/Rm of at least 0.7, the cold-rolled steel product consisting of a steel comprising iron, unavoidable production impurities and (in wt. % ) C: 0.05 - 0.20%, Si: 0.25 - 1.00%, Mn: 1.0 - 3.0%, Al : 0.02 - 1.5%, Cr: 0.1 - 1.5%, N: less than 0.02%, P: less than 0.03%, S: less than 0.05% and optionally one or more elements from the group "Ti, Mo, Nb, V, B" subject to Ti: being up to 0.15%, Mo: less than 2%, Nb: less than 0.1%, V: less than 0.12%, and B: 0.0005 - 0.003%. According to the invention the cold-rolled flat steel product provided undergoes additional heat treatment, during which it is annealed for an annealing time of 4.5 - 24 hours at an annealing temperature of up to 150 - 400°C. It has surprisingly transpired that as a result of such long-time annealing carried out at comparatively low temperatures a dramatic increase in the yield strength Re and an improvement in the hole expansion occurs. The invention also provides a cold rolled flat steel product consisting of the steel mentioned before and having a structure comprising at least two phases, which (in vol.-%) contains at least 10% tempered martensite, less than 10 % bainite, less than 10 % residual austenite and as the remainder ferrite, the steel having a yield ratio Re/Rm of at least 0.7, a tensile strength R of more than 750 MPa and a hole expansion LA of at least 18%.
机译:本发明提供了一种生产屈服比Re / Rm至少为0.7的冷轧钢带的方法,所述冷轧钢产品由包含铁,不可避免的生产杂质和(以重量%)C的钢组成: 0.05-0.20%,Si:0.25-1.00%,Mn:1.0-3.0%,Al:0.02-1.5%,Cr:0.1-1.5%,N:小于0.02%,P:小于0.03%,S:小于小于0.05%,并且可选地选自“ Ti,Mo,Nb,V,B”组中的一种或多种元素,其中Ti:至多0.15%,Mo:小于2%,Nb:小于0.1%,V:小于小于0.12%,而B:0.0005-0.003%。根据本发明,对所提供的冷轧扁钢产品进行额外的热处理,在此过程中,在最高150-400°C的退火温度下退火4.5至24小时的退火时间。令人惊奇地发现,由于在相对较低的温度下进行了这种长时间的退火,屈服强度Re显着增加,并且孔扩展得到改善。本发明还提供一种冷轧扁钢产品,该冷轧扁钢产品由前述钢组成并且具有包含至少两相的结构,该相包含(以体积计)至少包含10%的回火马氏体,少于10%的贝氏体,少于该钢的屈服比Re / Rm至少为0.7,抗拉强度R大于750 MPa,扩孔率LA至少为18%,残余奥氏体为10%,铁素体为残余。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号