The present invention relates to vitrification of radioactive waste. According to the present invention, the present invention provides a vitrification composition, proper for mixed waste in which combustible waste such as gloves, working clothes, and rubber products and low-radioactive waste are mixed; and a method for vitrifying the mixed waste using the same. According to the present invention, not only the volume of radioactive waste can substantially reduced but also release of radioactive materials in vitrified waste form can be delayed as long as possible or is completely prevented by vitrifying the mixed waste with the vitrification composition proper for vitrifying the mixed waste. The vitrification composition includes 40-50 wt% of SiO_2, 11-16 wt% of Al_2O_3, 8-15 wt% of B_2O_3, 3-6 wt% of CaO, 1-3 wt% of K_2O, 1-3 wt% of Li_2O, 1-3 wt% of MgO, 15-19 wt% of Na_2O, 0.5-3 wt% of TiO_2, 0.5-3 wt% of VO_2, 0.5-3 wt% of As_2O_5, 0.5-3 wt% of CeO_2, 0.1-2 wt% of CoO, 1-3 wt% of Fe_2O_3, 0.001-0.1 wt% of MnO_2, 0.1-1.0 wt% of P_2O_5, and 0.5-3 wt% of ZrO--_2.;COPYRIGHT KIPO 2015
机译:本发明涉及放射性废物的玻璃化。根据本发明,本发明提供一种适用于混合废弃物的玻璃化组合物,其中将手套,工作服,橡胶制品等可燃性废弃物与低放射性废弃物混合。以及使用该方法使混合废料玻璃化的方法。根据本发明,不仅可以大大减少放射性废物的体积,而且可以尽可能长地延迟或完全防止通过以适合于玻璃化的玻璃化组合物对混合废物进行玻璃化来完全防止玻璃化废物形式的放射性物质的释放。混合废物。玻璃化组合物包含40-50 wt%的SiO_2、11-16 wt%的Al_2O_3、8-15 wt%的B_2O_3、3-6 wt%的CaO,1-3 wt%的K_2O,1-3 wt%的Li_2O,1-3 wt%的MgO,15-19 wt%的Na_2O,0.5-3 wt%的TiO_2、0.5-3 wt%的VO_2、0.5-3 wt%的As_2O_5、0.5-3 wt%的CeO_2, CoO的0.1-2 wt%,Fe_2O_3的1-3 wt%,MnO_2的0.001-0.1 wt%,P_2O_5的0.1-1.0 wt%和ZrO --_ 2的0.5-3 wt%.; COPYRIGHT KIPO 2015

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号