ECO-FRIENDLY WOOD PLASTIC COMPOSITE PELLET WITH IMPROVED BIODEGRADABILITY AND METHOD FOR MANUFACTURING SAME

机译:具有改善的生物可降解性的生态友好型木塑复合材料球粒及其制造方法

摘要

According to the present invention, a method for manufacturing a eco-friendly wood plastic composite pellet with improved biodegradability comprises: (a) a mixing step of mixing, with an additive by stirring in a heat stirrer under a temperature of 90-110°C at a predetermined rotary velocity, 50-60 wt% of wood powder which has a particle size of 40-120 mesh and moisture content of 2-6%; 20-30 wt% of resin which consists of polypropylene and high-density polyethylene; 10-20 wt% of biodegradable mixed powder which consists of rice bran powder separated during the process of milling brown rice into rice and of fermentation accelerator prepared by adding quicklime to iron sulfate and heating the resultant material; and 3-10 wt% of calcium carbonate; and (b) a pellet extrusion step of injecting the mixture into a pellet extruder and extruding the mixture through cutting screws of the pellet extruder.;COPYRIGHT KIPO 2015
机译:根据本发明,一种具有改善的生物降解性的生态友好型木塑复合颗粒的制造方法包括:(a)在90-100℃的温度下通过在加热搅拌器中搅拌而与添加剂混合的混合步骤。在预定的转速下,木粉的50-60重量%,其粒度为40-120目,水分含量为2-6%; 20-30%(重量)由聚丙烯和高密度聚乙烯组成的树脂; 10-20wt%的可生物降解的混合粉末,其由在糙米碾磨成米的过程中分离的米糠粉和通过将生石灰添加到硫酸铁中并加热所得材料制备的发酵促进剂组成;和3-10重量%的碳酸钙; (b)将混合物注入颗粒挤出机中并通过颗粒挤出机的切割螺杆将混合物挤出的颗粒挤出步骤。COPYRIGHTKIPO 2015

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号