1. A method of manufacturing multilayer building blocks, comprising forming layers of the laminated wall block, including at least one external, at least one inner layer, if necessary, between the outer and inner layers are made further intermediate layer or intermediate layers, each layer made from mixtures whose composition comprises the following ingredients: concrete block, including crushed to the size of partitions of not less than 1 mm in an amount not less than 50% or expanded clay fractions with a grain size of not m than 1 mm and not less than 50%, any possible fractions the composition in an amount of cement is at least 20%, plasticizer in an amount of not less than 0.5%, the rest - water, respectively, in the manufacture of mixtures for the outer layer of the multilayer wall block is used, including expanded clay - at least 50% cement - at least 20%, plasticizer - not less than 0.5%, water - the rest, for the manufacture of the intermediate layer laminated wall block used, including expanded clay with various fractions with the size fractions at least 1 mm - at least 50% cement - at least 2 0%, plasticizer - not less than 0.5%, water - the rest, for the manufacture of an inner layer laminated wall block used, including sand - not less than 50% cement - at least 20%, plasticizer - not less than 0.5 %, water - the rest, selected quantities of ingredients for the layers of mixtures selected dimensional parameters block size parameters block layers, including length, width, thickness, shape and configuration of the laminated block, and the length, width, thickness, shape and configuration of each a layer for providing strength characteristics produced
机译:1。一种制造多层建筑砌块的方法,包括形成所述层压壁砌块的层,包括至少一个外部的,至少一个内层,如果需要的话,在所述外层和内层之间形成另外的一个或多个中间层,每个由混合物组成的一层,其组成包括以下成分:混凝土砌块,包括压碎至不少于1mm的隔板尺寸(不少于50%)或膨胀的粘土级分,其晶粒尺寸不少于1mm,以及在制造外层混合物的过程中,水泥含量不少于50%,水泥中任何可能的分数至少为20%,增塑剂含量不少于0.5%,其余为水。使用多层墙砖,包括膨胀粘土-至少50%水泥-至少20%,增塑剂-不小于0.5%,水-其余,用于制造中间层层压墙砖,包括各种分数的膨胀粘土,其大小分数至少为1毫米-水泥至少为50%-至少为2 0%,增塑剂-不少于0.5%,水-其余部分,用于制造内层层压墙砖使用,包括沙子-水泥含量不少于50%-至少20%,增塑剂-含量不少于0.5%,水-其余的,用于混合物层的选定成分数量选择的尺寸参数块尺寸参数块层,包括长度,层压块的宽度,厚度,形状和构造,以及每个提供强度特性的层的长度,宽度,厚度,形状和构造

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号