1. A process for the flotation of iron-containing minerals tungsten gravitational tailings comprising desliming initial pulp slurry conditioning with soda ash and the sodium soap of the fatty acid collector, tall oil example, at a pulp density of 30% solids and tungsten flotation of minerals, characterized in that, before feeding sodium soap fatty acid collector, together with soda ash, an aqueous solution of sodium hydroxide, and the flotation water is carried out at a temperature from 20 ° C to 8 ° C.2. A method according to claim 1, characterized in that the ratio of soda ash, caustic soda and sodium fatty acid soap is from collector 500:. 150: 200 to 500: 250: 200.
机译:1.一种浮选含铁矿物钨重力尾矿的方法,包括用苏打灰和脂肪酸收集剂的钠皂,例如妥尔油,以30%固体的纸浆密度脱泥初始的纸浆淤浆,并进行浮选。矿物,其特征在于,在馈入钠皂脂肪酸收集剂之前,与苏打粉,氢氧化钠水溶液和浮选水一起在20℃至8℃的温度下进行。 2.根据权利要求1所述的方法,其特征在于,纯碱,苛性苏打和脂肪酸钠皂的比例来自收集器500:。 150:200至500:250:200。

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号