FIELD: process engineering.;SUBSTANCE: set of inventions relates to production of construction materials and can be used for production of Portland cement clinker. This process comprises preheating of cement stock to temperature 600-800°C, glazing at 700-1000°C and annealing in rotary kiln at 1400-1500°C. Annealing is performed in parallel flow of cement stock and fuel followed by adsorption of sulphur oxides, alkaline metal oxides and chlorides from pre-cooled flue gases by clinker particles at 100-1100°C. In compliance with first version, adsorption is conducted partially at the annealing kiln end zone and partially in clinker cooler. In compliance with second version, pre-cooling and glazing are conducted in appropriate zones of annealing kiln. Adsorption is conducted partially at the annealing kiln end zone and partially in clinker cooler. In compliance with third version, cooling of flue gases and adsorption are conducted at appropriate temperature zones of annealing kiln. In compliance with fourth version, pre-cooling, glazing, flue gas cooling and adsorption are conducted in appropriate temperature zones. Invention is developed in dependent claim.;EFFECT: sufficient quality of cement, ruled out alkaline, chloride and hydrochloric contamination and emission of harmful substances.;26 cl, 6 dwg
机译:技术领域:工艺发明:一组发明涉及建筑材料的生产,并且可用于生产波特兰水泥熟料。此过程包括将水泥原料预热至600-800°C,在700-1000°C上釉以及在1400-1500°C的回转窑中退火。退火在水泥原料和燃料的平行流中进行,然后在100-1100°C下由熟料颗粒吸附来自预冷烟道气中的硫氧化物,碱金属氧化物和氯化物。根据第一版,吸附部分在窑尾区进行,部分在熟料冷却器中进行。根据第二版的规定,在退火窑的适当区域进行预冷和上光。吸附部分在窑尾端进行,部分在熟料冷却器中进行。根据第三版,在退火窑的适当温度区域进行烟气的冷却和吸附。根据第四版的规定,在适当的温度范围内进行预冷,上光,烟道气冷却和吸附。发明是从属权利要求中提出的;效果:足够的水泥质量,排除了碱,氯化物和盐酸的污染以及有害物质的排放。26cl,6 dwg

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号