FIELD: metallurgy.SUBSTANCE: method of production of seamless hot-worked boiler and steam line 530×30 - 75 mm pipes from "10?9?3?2????-?" grade refractory steel is characterized in that pipes are produced by melting using electroslag remelting of the hollow ingots 660×in.260-280×2100±50 mm, turning and boring to hollow cakes with size 640×in.280-360×2100±50 mm, heating of the cakes to temperature 1210-1230°C, piercing-rolling of the cakes in the helical rolling mills to shells with size 660×in.505-415×3350-2800 mm, shells rolling at Pilger mills to pipes 530×30-75×6700-3500 mm, cutting by hot cutting saw of the process wastes, straightening, heat treatment, etching, ultrasound testing and pipes acceptance.EFFECT: reduction of metal consumption and increased capacity of tube-forming installation with pilger mills.1 tbl
机译:领域:冶金学:从“ 10?9?3?2 ????-?”生产无缝热加工锅炉和蒸汽管线530×30-75 mm管道的方法优质耐火钢的特征在于,通过电渣重熔空心锭660×in.260-280×2100±50 mm,然后将其镗孔成640×in.280-360×2100±尺寸的空心饼,来制造管材50毫米,将饼加热到1210-1230°C的温度,在螺旋轧机中将饼冲孔轧制成尺寸660×in.505-415×3350-2800毫米的壳,壳在Pilger轧机轧制到管道530×30-75×6700-3500 mm,通过热切割锯切割工艺废料,矫直,热处理,蚀刻,超声测试和管道验收效果:减少金属消耗并增加使用皮尔格的成管设备的能力mills.1桶

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号