FIELD: chemistry.;SUBSTANCE: invention relates to obtaining granulated without binding agent zeolite of NaY type. Method includes mixing kaolin with powder-like zeolyte of NaY type, polyvinyl alcohol and component, selected from white soot, milled wide-pore silicagel or aerosil. Content of initial components in mixture constitutes:, wt %: powder-like zeolite of NaY type 55-70, polyvinyl alcohol 1-2, white soot or milled wide-pore silicagel, or aerosol 3-7, kaolin - the remaining part. After mixing carried out are: moisturising mixture until homogeneous mass is obtained, formation of granules, thermal activation, hydrothermal crystallisation in solution of sodium silicate, washing and drying of granules. Reaction mixture at crystallisation stage has the following molar composition : (2,2-2,6)Na2O·Al2O3·(6,5-7,5)SiO2·(155-165)H2O.;EFFECT: invention provides obtaining zeolite, possessing high phase purity, crystallinity degree, dynamic adsorption capacity, mechanical strength.;1 tbl, 12 ex
机译:发明领域本发明涉及获得没有NaY型粘合剂的粒化的粒状。方法包括将高岭土与NaY型粉末状沸石,聚乙烯醇和选自白烟灰,研磨的宽孔硅胶或气凝胶的组分混合。混合物中初始成分的含量为:wt%:NaY型55-70的粉末状沸石,聚乙烯醇1-2,白烟灰或研磨的宽孔硅胶或气溶胶3-7,高岭土-其余部分。混合后进行以下步骤:润湿混合物直至获得均匀的团块,形成颗粒,热活化,在硅酸钠溶液中水热结晶,洗涤并干燥颗粒。结晶阶段的反应混合物具有以下摩尔组成:(2,2-2,6)Na 2 O·Al 2 O 3 · (6,5-7,5)SiO 2 ·(155-165)H 2 O .;效果:本发明提供了一种具有高相纯度,结晶度的沸石,动态吸附能力,机械强度。; 1 tbl,12 ex

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号