PROBLEM TO BE SOLVED: To provide an inexpensive material having excellent hydrogen embrittlement resistance, tensile property and corrosion resistance.;SOLUTION: There is provided a non-magnetic corrosion resistant steel material which contains, by mass%, C:0.15 to 1.00%, Si:0.15 to 0.80%, Mn:6.0 to 10.0%, P:0.050% or less, S:0.030% or less, Ni:5.0 to 16.0%, Cr:8.0 to 15.0%, Cu:0.20 to 0.65%, V:0.30 to 2.00%, N:0.0150 to 0.1000% and the balance Fe with inevitable impurities, and which is excellent in hydrogen embrittlement resistance and mechanical properties, and in which a deposit composed of V (C, N) is 1 to 50 nm and V/{4([C]+[N])}=0.50 to 1.00, {16([C]+[N])-3[V]}/([Cr]+0.9[Ni]-16[N])}=0.075 to 0.250, 551-462([C]+[N]-0.07[V])-9.2[Si]-8.1[Mn]-13.7[Cr]-29([Ni]+[Cu])-18.5[Mo]≤-40.;SELECTED DRAWING: None;COPYRIGHT: (C)2017,JPO&INPIT
机译:解决的问题:为了提供一种廉价的材料,其具有优异的耐氢脆性,拉伸性能和耐腐蚀性。解决方案:提供了一种非磁性耐腐蚀钢材,该钢材的质量百分比为C:0.15至1.00%, Si:0.15〜0.80%,Mn:6.0〜10.0%,P:0.050%以下,S:0.030%以下,Ni:5.0〜16.0%,Cr:8.0〜15.0%,Cu:0.20〜0.65%,V :0.30〜2.00%,N:0.0150〜0.1000%,余量的Fe具有不可避免的杂质,耐氢脆性及机械特性优异,由V(C,N)构成的沉积物为1〜50nm。和V / {4([C] + [N])} = 0.50至1.00,{16([C] + [N])-3 [V]} /([Cr] +0.9 [Ni] -16 [ N])} = 0.075至0.250,551-462([C] + [N] -0.07 [V])-9.2 [Si] -8.1 [Mn] -13.7 [Cr] -29([Ni] + [Cu ])-18.5 [Mo]≤-40.;选定的图纸:无;版权:(C)2017,日本特许厅&INPIT

著录项

  • 公开/公告号JP2016183372A

    专利类型

  • 公开/公告日2016-10-20

    原文格式PDF

  • 申请/专利权人 SANYO SPECIAL STEEL CO LTD;

    申请/专利号JP20150063381

  • 发明设计人 HOSODA TAKASHI;

    申请日2015-03-25

  • 分类号C22C38/00;C22C38/58;C21D8/06;C21D6/00;

  • 国家 JP

  • 入库时间 2022-08-21 14:47:01

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号