首页> 外国专利> METHOD FOR PRODUCING MICROPOROUS MEMBRANE OR MICROPOROUS STRETCHED FILM, AND MICROPOROUS FILM OR MICROPOROUS BIAXIALLY STRETCHED FILM

METHOD FOR PRODUCING MICROPOROUS MEMBRANE OR MICROPOROUS STRETCHED FILM, AND MICROPOROUS FILM OR MICROPOROUS BIAXIALLY STRETCHED FILM

机译:制备微孔膜或微孔拉伸膜的方法,以及微孔膜或微孔双轴拉伸膜

摘要

PROBLEM TO BE SOLVED: To provide a method for obtaining a chemically modified cellulose nanofiber (chemically modified CeNF) reinforced microporous membrane which has a high void ratio and excellent air permeability, and has improved dynamic physical properties and heat resistance.SOLUTION: A method for producing a microporous membrane or a microporous stretched film includes: preparing a resin composition which contains polypropylene (PP) as a resin component, and contains 0.01-10 pts.wt. of chemically modified CeNF and 0.01-3 pts.wt. of a β crystal-nucleating agent, with respect to 100 pts.wt. of the resin component; melting and forming the resin composition into a film-like object where a crystal phase of a polypropylene component in the resin composition is substantially a β crystal phase, and a β-crystallization forming ability is preferably 70% or more; and then stretching the film-like object at a temperature of 90-155°C.SELECTED DRAWING: None
机译:解决的问题:提供一种获得化学改性的纤维素纳米纤维(化学改性的CeNF)增强的微孔膜的方法,该膜具有较高的空隙率和优异的透气性,并具有改善的动态物理性能和耐热性。制备微孔膜或微孔拉伸膜的步骤包括:制备包含聚丙烯(PP)作为树脂组分并且包含0.01-10 pts.wt的树脂组合物。化学修饰的CeNF和0.01-3 pts.wt.相对于100 pts.wt的β晶体成核剂树脂成分;将所述树脂组合物熔融而形成为膜状,其中,所述树脂组合物中的聚丙烯成分的结晶相实质上为β结晶相,β结晶形成能力优选为70%以上。然后在90-155°C的温度下拉伸薄膜状物体。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号