PROBLEM TO BE SOLVED: To provide: a high-fluidity lightweight mortar composition which is light and excellent in fluidity, does not cause bleeding or material separation, is suppressed in swelling after working as a filler for a steel plate lining construction method, has good workability, and exerts sufficient strength; and a high-fluidity lightweight mortar using the same.SOLUTION: A high-fluidity lightweight mortar composition comprises: cement; a blast furnace fine slag powder of a Blaine specific surface area exceeding 6,000 cm/g; an expansive material; light aggregate with a density of 0.1-0.7 kg/l; and a water-soluble cellulosic thickener and an acrylic thickener, but contains no water-reducing agent. The high-fluidity lightweight mortar composition contains 20-70 pts. mass of the cement, 25-75 pts. mass of the blast furnace slag fine powder and 2-10 pts. mass of the expansive material in 100 pts. mass of the binding material consisting of the cement, the blast furnace slag fine powder and the expansive material.
机译:解决的问题:提供:一种轻质且流动性优异,不引起渗出或材料分离,在用作钢板衬砌施工方法的填充剂后被抑制溶胀的高流动性轻质砂浆组合物,具有良好的性能。可加工性,并发挥出足够的强度;解决方案:高流动性轻质砂浆组合物包含:水泥; Blaine比表面积超过6,000 cm / g的高炉细渣粉;膨胀材料;轻骨料,密度为0.1-0.7 kg / l;水溶性纤维素增稠剂和丙烯酸增稠剂,但不包含减水剂。高流动性轻质砂浆组合物含量为20-70分。水泥质量,25-75分。高炉矿渣细粉的质量为2-10点。膨胀材料的质量(100磅)。由水泥,高炉矿渣细粉和膨胀材料组成的粘结材料的质量。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号