首页> 外国专利> It is played completely hydrogenate the catalyst effect on the aromatic ring, a manufacturing method of a supported ultrafine amorphous metallic nickel catalyst

It is played completely hydrogenate the catalyst effect on the aromatic ring, a manufacturing method of a supported ultrafine amorphous metallic nickel catalyst

机译:它发挥了完全加氢催化对芳环的作用,一种负载型超细非晶态金属镍催化剂的制备方法

摘要

to really fully hydrogenated a catalyst effect on the aromatic ring, to provide a method for producing a supported type of ultra-fine amorphous metallic nickel catalyst. High pressure reactor lid is opened, in turn, the organic solvent 10 to 1000 (ml), the catalyst support 1-4 g, after adding nickel carbonyl 1 to 100 (ml), close the upper cover. High-purity nitrogen gas was gradually flows into the gas inlet flows out from the gas outlet, until the pressure becomes 2 8MPa, high purity hydrogen gas, gradually introduced into the high pressure reactor via the gas inlet , then, shut the gas inlet valve. By starting the motor drives the magnetic stirrer, after thoroughly stirring and mixing at room temperature, at a fast agitation speed, temperature is rapidly heated until the 70~280 , and keep warm. Nickel carbonyl adsorbed on the surface of the carrier is decomposed to the elemental nickel and the nickel alone is deposited on the surface of the carrier. This, to be really fully hydrogenated a catalyst effect on the aromatic ring, but to produce a supported type of ultra-fine amorphous metallic nickel catalyst.FIELD 1
机译:本发明提供了一种制备负载型超细非晶态金属镍催化剂的方法。打开高压反应器的盖子,依次将有机溶剂10到1000(ml),催化剂载体1-4 g,加入羰基镍1到100(ml)后,关闭上盖。高纯氮气逐渐流入进气口,从出气口流出,直到压力变为2 8MPa,高纯氢气通过进气口逐渐引入高压反应器,然后,关闭进气阀。在室温下充分搅拌混合后,通过启动电动机来驱动磁力搅拌器,将温度迅速加热至70〜280℃,并保持温暖。吸附在载体表面上的羰基镍分解为元素镍,仅镍沉积在载体表面上。这实际上是完全氢化了对芳环的催化剂作用,但制得了负载型超细无定形金属镍催化剂。FIELD1

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号