A reaction system comprising an organic polyisocyanate and an isocyanate reactive component for preparation of a viscoelastic polyurethane foam is provided. The isocyanate reactive component comprises (i) from 10 to 50% by weight of one or more low equivalent weight propylene oxide rich (PO-rich) polyols having a combined number average equivalent weight from 200 to 500, (ii) from 45 to 95% by weight of one or more ethylene oxide (EO-rich) polyols having a combined number average equivalent weight from 200 to 800 and an ethylene oxide content from 40% to 65% by weight of the total mass of the EO-rich polyol and at least one of (iii) from 10 to 30% by weight of one or more high equivalent weight PO-rich polyols having a number average equivalent weight from 800 to 2,000 or (iv) from 10 to 40% by weight of one or more propylene oxide co-polymer polyols containing styrene-acrylonitrile.
机译:提供了一种用于制备粘弹性聚氨酯泡沫的包含有机多异氰酸酯和异氰酸酯反应性组分的反应体系。异氰酸酯反应性组分包含(i)按重量计10%至5​​0%的一种或多种低数均环氧丙烷(富PO)多元醇,其合计数均当量为200至500,(ii)45至95。数均当量为200至800的环氧乙烷(富EO)多元醇的总重量百分比,按重量计,一种或多种环氧乙烷(富EO)多元醇的总质量为40%至65%。 (iii)10至30重量%的一种或多种数均当量为800至2,000的高当量重富PO多元醇或(iv)10至40 wt%的一种或多种中的至少一种含有苯乙烯-丙烯腈的环氧丙烷共聚物多元醇。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号