首页> 外国专利> Method of manufacturing a bonded joint of the friction stir welding method and the structural steel of structural steel

Method of manufacturing a bonded joint of the friction stir welding method and the structural steel of structural steel

机译:摩擦搅拌焊接法与结构钢的结构钢的接合接头的制造方法

摘要

Purposes of the invention is, when flowing backwards failure with advantageous way address, also improves connection construction since insufficient heating material to be processed carries out friction stir weld structural steel to provide enough intensity. In the present invention, the structural steel of agitating friction weldering is executed during the pre-heat treatment technique, the pre-heat treatment technique is a kind of process, its light plate (3), which is material to be treated heating, that movement direction of engagement in front of the rotation tool (1) provided by heating (5). The present invention is constructed such that surface temperature, surface area, position, etc. heating region, be strictly control in the preheating treatment procedure.
机译:本发明的目的是,当以有利的方式解决倒流故障时,由于待处理的加热材料不足而进行了摩擦搅拌焊接结构钢以提供足够的强度,因此还改善了连接构造。在本发明中,搅拌摩擦焊的结构钢是在预热处理技术中进行的,预热处理技术是一种工艺,其轻质板(3)是被加热处理的材料,加热(5)在旋转工具(1)前面接合的运动方向。本发明的构造使得在预热处理过程中严格控制表面温度,表面积,位置等加热区域。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号