首页> 外国专利> thermal cracking additive compounds for reducing coke yield in delayed coking processes

thermal cracking additive compounds for reducing coke yield in delayed coking processes

机译:热裂化添加剂化合物,用于降低延迟焦化过程中的焦炭收率

摘要

"Thermal cracking additive compounds for reducing coke yield in delayed coking processes", as the present invention is directed to novel thermal cracking additive compounds for reducing coke yield in delayed coking processes and a method of preparation of them. The present invention also provides that the thermal cracking additive compounds of the present invention have micro size and nano size. furthermore, the present invention discloses a thermal cracking process of heavy petroleum waste used in petroleum refineries using the delayed coking process for the production of petroleum coke and lighter hydrocarbon products with reduced coke yield and increased yield. of liquid and / or gaseous products.
机译:本发明涉及“用于在延迟的焦化过程中降低焦炭收率的热裂化添加剂化合物”,以及用于在延迟的焦化过程中降低焦炭收率的新型热裂化添加剂化合物。本发明还提供了本发明的热裂化添加剂化合物具有微米尺寸和纳米尺寸。此外,本发明公开了一种用于石油精炼厂的重质石油废料的热裂化方法,其使用延迟焦化工艺生产石油焦炭和较轻的烃产物,从而降低了焦炭收率并提高了收率。液体和/或气体产品。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号