The invention concerns a process for converting heavy feeds carried out in a slurry reactor in the presence of hydrogen and in the presence of a catalyst comprising at least one catalytic metal or a compound of a catalytic metal from group VIE and/or VIII supported on alumina, the pore structure of which is composed of a plurality of juxtaposed agglomerates each formed by a plurality of acicular platelets, the platelets of each agglomerate being generally radically oriented with respect to the others and with respect to the center of the agglomerate, said catalyst having an irregular and non-spherical shape and being mainly in the form of fragments, obtained using a process including the following steps: a) granulation starting from an active alumina powder having a low crystalline and/or amorphous structure, to obtain agglomerates in the form of beads; b) maturing in a moist atmosphere between 60°C and lOO then drying said beads; c) sieving to recover a fraction of said beads; d) crushing said fraction; e) calcining at least a portion of said crushed fraction at a temperature in the range 250°C to 900°C; f) impregnating with acid and hydrothermal treatment at a temperature in the range 80°C to 250°C; g) drying then calcining at a temperature in the range 500°C to 1100°C; h) depositing at least one catalytic metal or compound of a catalytic metal from group VIB and/or group VIII by impregnation. The process of the invention employs a catalyst with a specific pore texture, shape and granulometry, resulting in improved performances.
机译:本发明涉及在淤浆反应器中在氢气存在下和在催化剂上存在的转化重质进料的方法,所述催化剂包含至少一种负载在氧化铝上的VIE和/或VIII族催化金属或催化金属化合物,其孔结构由多个并置的附聚物组成,每个附聚物由多个针状血小板形成,每个附聚物的血小板通常相对于彼此和相对于附聚物的中心是自由基取向的,所述催化剂具有使用包括以下步骤的方法获得的不规则形状和非球形形状,并且主要为碎片形式:a)从具有低结晶度和/或无定形结构的活性氧化铝粉末开始制粒,以获得以下形式的附聚物珠子b)在60℃至100℃的潮湿气氛中熟化,然后干燥所述珠粒; c)筛分以回收一部分所述珠; d)粉碎所述级分; e)在250℃至900℃范围内的温度下煅烧至少一部分所述压碎的级分; f)在80℃至250℃的温度范围内用酸浸渍和水热处理; g)干燥,然后在500℃至1100℃的温度下煅烧; h)通过浸渍沉积来自VIB族和/或VIII族的至少一种催化金属或催化金属的化合物。本发明的方法使用具有特定孔质地,形状和粒度的催化剂,从而导致性能提高。

著录项

  • 公开/公告号IN275691B

    专利类型

  • 公开/公告日2016-09-23

    原文格式PDF

  • 申请/专利权人

    申请/专利号IN3056/CHE/2007

  • 发明设计人 ROY-AUBERGER MAGALIE;GUILLAUME DENIS;

    申请日2007-12-19

  • 分类号C10G47/00;

  • 国家 IN

  • 入库时间 2022-08-21 14:24:30

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号