首页> 外国专利> Method for producing zeolites on the basis of Filipowice volcanic tuff

Method for producing zeolites on the basis of Filipowice volcanic tuff

机译:基于Filipowice火山凝灰岩的沸石生产方法

摘要

method of manufacturing zeolite based on filipowickiego tofu wrap volcanic alkaline fusion method, using sodium hydroxide as activator zeolityzacji process, is that filipowicki tuff, schist before mixing with other components is chopped to grain size 10 - 800 mm, fragmented tuf mixed with constant sodium hydroxide in relation tuf / naoh = 0.5 - 0.9 and after ujednorodnieniu mixture spieka her at 400 - 650u00b0c, for 1 to 2 h, after cooling, is minced to grain size below 200 mm and is mixed with water, using for 1 g of solid material from 2 to 10 ml of water, after which the mixture is at a temperature of 80 to 120u00b0c, by 18 - 26 h.subsequently the mixture is held at a temperature of 40 - 80u00b0c, for 8 to 16 h, separates the solid product from liquid poreakcyjnej, washed him with demineralised water to obtain ph 8 - 11 and dried at 80 - 110u00b0c until constant weight.
机译:基于filipowickiego豆腐包裹的火山碱性熔融法制造沸石的方法,使用氢氧化钠作为活化剂zeolityzacji工艺,是将filipowicki凝灰岩,片岩在与其他组分混合之前切成10-800 mm的粒度,将碎屑与恒定的氢氧化钠混合相对于tuf / naoh = 0.5-0.9,在ujednorodnieniu混合物中以400-650 u00b0c混合spieka之后,冷却1至2 h,将其切成小于200 mm的粒度,并与水混合,使用1 g从2到10毫升水中加入固体物料,然后将混合物在80到120摄氏度的温度下放置18-26小时,然后将混合物在40-80摄氏度的温度下保持8到60摄氏度。 16小时,将固体产物与液体孔隙分离,用软化水洗涤,得到pH 8-11,并在80-110℃干燥至恒重。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号