The present invention provides a water-reducing agent for low-heating high-strength concrete formed of 50 to 70 wt% of maintainer and 30 to 50 wt% of water reducer as polycarboxylic acid, an alkali ion activation agent for low-heating high-strength concrete configured by mixing between 30 to 50 wt% of tri-ethanol-amine (TEA) and 50 to 70 wt% of polypenol-amine (PA), and a low-heating high-strength concrete composition configured to contain 450 to 550 kg/m^3 of binding material (B) formed of 45 to 55 wt% of blast furnace slag fine powder, 25 to 35 wt% of ordinary Portland cement, and 15 to 25 wt% of fly ash; 135 to 175 kg/m^3 of water (W); 700 to 770 kg/m^3 of fine aggregate (S); 850 to 940 kg/m^3 of coarse aggregate (G); 4.05 to 8.25 kg/m^3 of the water-reducing agent for low-heating high-strength concrete; and the alkali ion activation agent for low-heating high-strength concrete, in which the water-binding material ratio (W/B) is 27 to 35% and the fine aggregate ratio (S/a) is 42 to 48%, 0.9 to 1.4 parts by weight of the water-reducing agent for low-heating high-strength concrete is mixed with respect to 100 parts by weight of the binding material (B), and 0.1 part by weight of the alkali ion activation agent for low-heating high-strength concrete is mixed with respect to 100 parts by weight of the binding material (B).
机译:本发明提供了由50至70重量%的保持剂和30至50重量%的减水剂作为多元羧酸形成的用于低热高强度混凝土的减水剂,一种用于低热高强度混凝土的碱离子活化剂。通过混合30至50 wt%的三乙醇胺(TEA)和50至70 wt%的聚对苯二胺(PA)来配置的高强度混凝土,以及配置为包含450至550的低热高强度混凝土组合物kg / m ^ 3的粘结材料(B),由高炉矿渣细粉45至55 wt%,普通硅酸盐水泥25至35 wt%和粉煤灰15至25 wt%组成; 135至175 kg / m ^ 3的水(W); 700至770 kg / m ^ 3细骨料(S); 850至940 kg / m ^ 3粗骨料(G);用于低热高强度混凝土的减水剂为4.05至8.25 kg / m ^ 3;用于低热高强度混凝土的碱离子活化剂,其中水结合材料的比率(W / B)为27%至35%,细骨料比率(S / a)为42%至48%,0.9相对于100重量份的粘结材料(B)和0.1重量份的低离子强度的碱离子活化剂,将1.4重量份的低热高强度混凝土减水剂混合。相对于100重量份的粘结材料(B),混合加热的高强度混凝土。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号