INORGANIC LIGHTWEIGHT HEAT INSULATING COMPOSITION AND A MANUFACTURING METHOD OF INORGANIC LIGHTWEIGHT HEAT INSULATING MATERIAL CONTAINING THE SAME

机译:无机轻质隔热保温材料及其制造方法

摘要

The present invention relates to a lightweight foam inorganic insulation material composition in which a volume of independent foam in a volume of the total composition is 88-98%, density is 0.05-0.16 g/cm^3, and thermal conductivity is 0.032-0.050 W/mK by mixing an animal foaming agent, which is pre-foamed, and paste including 50-100 parts by weight of cement; 5-20 parts by weight of admixture, 1-50 parts by weight of a hardening accelerator; 0.01-2 parts by weight of a superplasticizer; 0.01-5 parts by weight of acrylic emulsion; 0.01-2 parts by weight of a foam enhancer; 0.01-1 parts by weight of a fiber; and 35-120 parts by weight of mixing water. In addition, autoclave curing is unnecessary unlike a conventional cement-based inorganic insulation material. Moreover, provided is a method of manufacturing a lightweight foam inorganic insulation material comprising: a step (a) of manufacturing paste including 50-100 parts by weight of cement, 5-20 parts by weight of admixture, 1-50 parts by weight of a hardening accelerator, 0.01-2 parts by weight of a superplasticizer, 0.01-5 parts by weight of acrylic emulsion, 0.01-2 parts by weight of a foam enhancer, 0.01-1 parts by weight of a fiber, and 35-120 parts by weight of mixing water; a step (b) of manufacturing a lightweight foam inorganic insulation material composition by mixing a foamed animal foaming agent and the paste to allow a volume of independent foam in a volume of the total composition to be 88-98%; and a step (c) of forming the lightweight foam inorganic insulation material composition, and curing the same at room temperature.
机译:本发明涉及一种轻质泡沫无机绝缘材料组合物,其中,在全部组合物中,独立泡沫的体积为88〜98%,密度为0.05〜0.16g / cm 3,热导率为0.032〜0.050。通过将预发泡的动物发泡剂与包含50-100重量份水泥的糊料混合,以W / mK混合; 5-20重量份的混合物,1-50重量份的硬化促进剂; 0.01-2重量份的高效减水剂; 0.01-5重量份丙烯酸乳液; 0.01-2重量份的泡沫增强剂; 0.01-1重量份的纤维;和35-120重量份的混合水。另外,与常规的基于水泥的无机绝缘材料不同,不需要高压釜固化。此外,提供了一种制造轻质泡沫无机绝缘材料的方法,该方法包括:步骤(a),制造包含50-100重量份的水泥,5-20重量份的混合物,1-50重量份的水泥的糊剂。硬化促进剂,0.01-2重量份的高效减水剂,0.01-5重量份的丙烯酸乳液,0.01-2重量份的泡沫增强剂,0.01-1重量份的纤维和35-120重量份按混合水的重量;步骤(b),通过混合泡沫动物发泡剂和糊剂以使独立泡沫在总组合物中的体积为88-98%来制造轻质泡沫无机绝缘材料组合物;形成轻质泡沫无机绝缘材料组合物并在室温下固化的步骤(c)。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号