1. A method for increasing the corrosion resistance of a metallic article having a surface machining products providing surface hardening and surface passivation izdeliya.2. The method of claim. 1, characterized in that the mechanical treatment is a mechanical polishing and / or shot blasting and / or gidrodrobestruynoy treatment and / or gidrogaltovke and / or vibrogaltovke or tumbled and / or mechanical grinding and / or knurled or running-roller and / or burnishing, and / or ultrasonic treatment of the surface of the microparticles izdeliya.3. The method of claim. 1, characterized in that the machining provides surface hardening with the degree of not less than 5% or 6% or 7%, or 8%, or 9% or 10% .4. The method of claim. 1, characterized in that the machining provides surface hardening depth of at least 8 microns, or 15 microns or 20 microns or 22 microns or 27 mkm.5. The method of claim. 1, characterized in that the surface passivation of the product is carried out in a gaseous medium and / or coolant containing oxygen and / or water par.6. The method of claim. 1, characterized in that the products provide surface passivation layer oxide film thickness of not less than 1.5 mkm.7. The method of claim. 1, characterized in that on the surface of the article a protective coating applied to metal, steel or alloys and / or doped izdeliya.8 surface. The method of claim. 7, characterized in that the surface doping of the product is a nitriding or carbonitriding poverhnosti.9. The method of claim. 1, characterized in that the heat treatment is carried articles and / or surfaces izdeliya.10. A metallic article having a surface with an arithmetic mean deviation of the profile Ra of less than 1.6 microns thick and oksidnog
机译:1.一种提高具有表面加工产品的金属制品的耐腐蚀性的方法,所述产品提供表面硬化和表面钝化处理。2。权利要求的方法。 1,其特征在于机械处理是机械抛光和/或喷丸处理和/或gidrodrobestruynoy处理和/或gidrogaltovke和/或vibrogaltovke或滚落和/或机械研磨和/或滚花或滚轮和/或抛光,和/或超声波处理izdeliya微粒的表面3。权利要求的方法。 1,特征在于机加工提供的表面硬化度不少于5%或6%或7%,或8%,或9%或10%.4。权利要求的方法。如图1所示,其特征在于机加工提供的表面硬化深度至少为8微米,或15微米或20微米或22微米或27mkm.5。权利要求的方法。 1,其特征在于产品的表面钝化是在气态介质和/或含氧和/或水的冷却剂中进行的(6段)。权利要求的方法。 1,特征在于该产品提供的表面钝化层的氧化膜厚度不小于1.5mkm.7。权利要求的方法。 1,特征在于在制品的表面上施加到金属,钢或合金和/或掺杂的izdeliya.8表面的保护涂层。权利要求的方法。 7,特征在于产品的表面掺杂是氮化或碳氮共渗。9。权利要求的方法。 1,其特征在于热处理是携带物品和/或表面izdeliya.10。一种金属制品,其表面的轮廓Ra的算术平均偏差小于1.6微米厚,并且oksidnog

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号