1. A rubber mixture, characterized in that it contains the cobalt compound in an amount in terms of parts by weight of cobalt 0,0025-0,05 per 100 parts by weight rubber komponenta.2. A method of manufacturing rubber composite article comprising: a surface treatment process by bringing the metallic material into contact with a buffer solution; and the process of mounting the rubber composition according to Claim. 1 to metallic materials subjected to a process poverhnosti.3 processing. A method of manufacturing rubber composite article according to claim. 2, wherein the pH buffer is 5,0-7,2.4. A method of manufacturing rubber composite article according to claim. 2 or 3, wherein the buffer solution is substantially free of transition metallov.5. A method of manufacturing rubber composite article according to claim. 2 or 3, wherein the buffer solution contains at least one kind of acid selected from acids with a dissociation constant (pKa) in the range of 4-8.6. A method of manufacturing rubber composite article according to claim. 4, wherein the buffer solution contains at least one kind of acid selected from acids with a dissociation constant (pKa) in the range of 4-8.7. Rubber-metal composite product made in accordance with the method for manufacturing a rubber composite article according to any one of claims. 2-6.8. A tire comprising a rubber-metal composite article according to claim. 7.9. The industrial belt comprising a rubber-metal composite article according to claim. 7.10. A rubber track comprising rubber-metal composite article according to claim. 7.
机译:1.一种橡胶混合物,其特征在于,以每100重量份的橡胶komponenta 2的重量份计,钴化合物的含量为0.0025-0.05。一种橡胶复合制品的制造方法,包括:通过使金属材料与缓冲溶液接触的表面处理工艺;以及根据权利要求1的橡胶组合物的安装方法。 1到金属材料进行了加工poverhnosti.3加工。 8.根据权利要求1的橡胶复合制品的制造方法。参照图2,其中pH缓冲剂为5,0-7,2.4。 8.根据权利要求1的橡胶复合制品的制造方法。参照图2或3,其中缓冲溶液基本上不含过渡金属。5。 8.根据权利要求1的橡胶复合制品的制造方法。参照图2或3,其中缓冲溶液包含选自解离常数(pKa)在4-8.6范围内的酸中的至少一种酸。 8.根据权利要求1的橡胶复合制品的制造方法。参照图4,其中缓冲溶液包含至少一种选自解离常数(pKa)在4-8.7范围内的酸。 7.根据权利要求1〜8中任一项所述的橡胶复合制品的制造方法制造的橡胶金属复合制品。 2-6.8。 11.一种轮胎,其包括根据权利要求1的橡胶-金属复合制品。 7.9。 7.一种工业皮带,其包括根据权利要求1所述的橡胶-金属复合制品。 7.10。 15.一种橡胶履带,其包含根据权利要求1的橡胶-金属复合制品。 7。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号