首页> 外国专利> Method of disposal of radioactive waste in 'synthetic rock'

Method of disposal of radioactive waste in 'synthetic rock'

机译:“合成岩”中放射性废物的处置方法

摘要

The invention relates to the disposal of radioactive waste by a modified sol-gel method by enclosing it in durable ceramic crystallographic structures of ceramic synroc materials of type perovskite.;The method according to the invention lies in the fact that to the previously prepared chlorine-free solution of colloidal sol, preferably Ti(NO3)4, the complexing compound is added, preferably ascorbic acid ASC, relative to the sum of the moles of metal from 0.1 to 0.3 and introduces calcium carbonate and elements included in the high-level radioactive waste, in the form of carbonates or nitrates, especially strontium, cobalt, cesium and neodymium, in a molar ratio of from 2% to 14% of the individual metals (Me), thereby replacing from 2% to 14% by mol of introduced Ca2+.The thus obtained sol is evaporated, dried and subjected to heat treatment and is eventually subjected to XRD and IR analysis, then the precursor of the synroc is pelletized and calcined at a temperature of 1200°C for 2h.
机译:本发明涉及通过将改进的溶胶-凝胶方法封闭在钙钛矿型陶瓷合成材料的耐用陶瓷晶体结构中而通过改进的溶胶-凝胶法处理放射性废物。根据本发明的方法在于以下事实:预先制备的氯-游离的胶体溶胶溶液,最好是Ti(NO 3 4 ,相对于金属摩尔总和,加入络合化合物,最好是抗坏血酸ASC到0.3,并以碳酸盐或硝酸盐的形式(特别是锶,钴,铯和钕)引入碳酸钙和高放射性废物中包含的元素,摩尔比占每种金属的2%至14%( Me),从而以2%到14%的摩尔比代替所引入的Ca 2 + 。将所得溶胶蒸发,干燥并进行热处理,最后进行XRD和IR分析,然后将synroc的前体制成颗粒并在90℃下煅烧在1200°C的温度下放置2小时。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号