Provided are: acrylic fibers having 2-7% boiling water shrinkage and formed by the side-by-side conjugation of a copolymer A, which contains 5-10 mass% of an unsaturated monomer that can form a copolymer with acrylonitrile units, and a copolymer B, which contains 2-5 mass% of unsaturated monomer units that can form a copolymer with acrylonitrile units and 0.2-1.5 mass% of sulfonic acid group-containing monomer units; a method for manufacturing said fibers; a spun yarn containing said fibers; and a knitted fabric obtained from said spun yarn. The single fiber fineness of the heat-treated acrylic fibers is 1.7-6.6 dtex, the bulkiness is at least 380 cm3/g, the percentage of crimp is at least 15%, and the product (DKSDKE) of the knot strength (cN/dtex) and the knot elongation (%) is 10-25. The acrylic fibers have excellent crimp characteristics and anti-pilling properties.
机译:提供:具有2-7%沸水收缩率并且通过并排共轭共聚物A而形成的丙烯酸类纤维,所述丙烯酸类纤维包含5-10质量%的可以与丙烯腈单元形成共聚物的不饱和单体。共聚物B,其包含2-5质量%的可与丙烯腈单元形成共聚物的不饱和单体单元和0.2-1.5质量%的含磺酸基的单体单元;制造所述纤维的方法;包含所述纤维的细纱;由上述细纱获得的针织物。热处理丙烯酸纤维的单纤维纤度为1.7-6.6 dtex,蓬松度至少为380 cm3 / g,卷曲率至少为15%,结强度(cN / m)的乘积(DKSDKE) dtex)和结伸长率(%)为10-25。丙烯酸纤维具有优异的卷曲特性和抗起球性。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号