首页> 外国专利> STEEL STRIP NOTCHING EQUIPMENT, STEEL STRIP NOTCHING METHOD, COLD ROLLING FACILITY, COLD ROLLING METHOD, AND MANUFACTURING METHOD OF COLD ROLLING STEEL STRIP

STEEL STRIP NOTCHING EQUIPMENT, STEEL STRIP NOTCHING METHOD, COLD ROLLING FACILITY, COLD ROLLING METHOD, AND MANUFACTURING METHOD OF COLD ROLLING STEEL STRIP

机译:钢带刻痕设备,钢带刻痕方法,冷轧设备,冷轧方法以及冷轧钢带的制造方法

摘要

PROBLEM TO BE SOLVED: To provide steel strip notching equipment, a steel strip notching method, a cold rolling facility, a cold rolling method, and a manufacturing method of a cold rolling steel strip that enable cold rolling without causing a joint part rupture (weld zone rupture) even in a brittle material and a high alloy material such as a silicon steel sheet and a high-tensile steel sheet with high contents of Si and Mn.SOLUTION: Steel strip notching equipment for forming a notch in a plate width direction end portion of a joint part where the rear end of a preceding steel strip and the leading end of a succeeding steel strip are joined includes notching means that causes an amount of increase in Vickers hardness in a plate end after the notch formation to be less than Hv 50 as compared to before the notch formation, and causes an amount of dross formation to be 0.2 mm or less.SELECTED DRAWING: Figure 7
机译:解决的问题:提供一种带钢开槽设备,带钢开槽方法,冷轧设备,冷轧方法以及能够进行冷轧而不会引起接头部破裂的冷轧钢带的制造方法(焊接)。甚至在硅和锰含量高的硅钢片和高强度钢板等脆性材料和高合金材料中也发生断裂)。解决方案:用于在板宽方向端部形成缺口的钢带缺口设备将前一条钢板的后端和后一条钢板的前端连接在一起的接头部分的一部分,包括切槽,使切槽形成后的板端的维氏硬度增加量小于Hv。与切口形成之前相比为50,并且导致渣causes形成量为0.2 mm或更小。图7

著录项

  • 公开/公告号JP2017080803A

    专利类型

  • 公开/公告日2017-05-18

    原文格式PDF

  • 申请/专利权人 JFE STEEL CORP;

    申请/专利号JP20160120575

  • 申请日2016-06-17

  • 分类号B21B15;B21B1/22;B23K26/38;B23H9;B23H9/02;B23K31;

  • 国家 JP

  • 入库时间 2022-08-21 14:01:43