PREPARATION METHOD OF HIGH-EARLY-STRENGTH CONCRETE AND CURED BODY

机译:高强混凝土及空心砌体的制备方法

摘要

PROBLEM TO BE SOLVED: To provide a preparation method of a high-early-strength concrete promoting aggregation and curing at early time by stopping flowability quickly when filling of parts is completed sequentially while maintaining flowability during filling operation and a cured body thereof for overcoming problems that there is need for constructing a frame having a sufficient framework in a concrete construction for filling and installing concrete excellent in flowability and cost and labor are required for the operation and there is need for shortening construction period of the concrete construction.;SOLUTION: There is provided a preparation method of a high-early-strength concrete, including mixing a concrete of a base blend and then adding, to the concrete slurry, a predetermined amount of an admixture composition containing, at a specific ratio, constitutional components containing A component:one or more selected from specific polyacrylamide and specific polyacrylic acid alkali metal salt, B component: silicate alkali metal salt, C component: specific polyalkylene glycol monoalkyl ether, D component: sodium phosphate, and E component: water.;SELECTED DRAWING: None;COPYRIGHT: (C)2017,JPO&INPIT
机译:解决的问题:提供一种高强度混凝土的制备方法,该方法通过在顺序完成零件的填充时迅速停止流动性,同时在填充操作过程中保持流动性,从而在早期阶段促进凝结和固化,从而克服了问题。需要在混凝土结构中构造具有足够框架的框架以填充和安装流动性和成本优异的混凝土,并且操作需要人工,并且需要缩短混凝土结构的建造周期。提供一种高早强混凝土的制备方法,该方法包括混合基础混合料的混凝土,然后向该混凝土浆中加入预定量的掺混剂组合物,该掺混剂组合物以特定比例包含含有A成分的组成成分。 :选自特定的聚丙烯酰胺和特定的聚丙烯酸碱中的一种或多种锂金属盐,B组分:硅酸盐碱金属盐,C组分:特定的聚亚烷基二醇单烷基醚,D组分:磷酸钠,E组分:水。;部分制图:无;版权:(C)2017,JPO&INPIT

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号