MODIFIED ASPHALT COMPOSITION AND MODIFIED ASPHALT MIXTURE, AND METHOD FOR PRODUCING THEM

机译:改性沥青组合物和改性沥青混合物及其制备方法

摘要

PROBLEM TO BE SOLVED: To provide a modified asphalt composition and a modified asphalt mixture excellent in fluidity resistance, aggregate peeling resistance, compatibility and high temperature storage stability (heat resistance), and to provide a method for producing them.;SOLUTION: There is provided a modified asphalt composition which contains 0.5-20 pts.mass of a block copolymer (B) with respect to 100 pts.mass of asphalt (A), and 0.5-20 pts.mass of an additive (C) containing at least one selected from the group consisting of a tackifier resin, oil and a crosslinking agent, where the block copolymer (B) contains at least a vinyl aromatic monomer unit and a conjugated diene monomer unit, a content of the vinyl aromatic monomer unit contained in the block copolymer (B) is 33-60 mass%, and a peak temperature of a loss tangent (tanδ) by dynamic viscoelasticity measurement of the block copolymer (B) is -50°C or higher and -5°C or lower.;SELECTED DRAWING: None;COPYRIGHT: (C)2017,JPO&INPIT
机译:要解决的问题:提供一种具有优异的耐流动性,集料抗剥离性,相容性和高温储存稳定性(耐热性)优异的改性沥青组合物和改性沥青混合物,并提供一种生产方法。提供了一种改性沥青组合物,相对于100 pts。质量的沥青(A)包含0.5-20 pts。质量的嵌段共聚物(B)和0.5-20 pts。质量的添加剂(C),其中至少一种选自由增粘树脂,油和交联剂组成的组中的嵌段共聚物(B)至少包含乙烯基芳族单体单元和共轭二烯单体单元,嵌段中包含的乙烯基芳族单体单元的含量共聚物(B)为33〜60质量%,通过动态粘弹性测定法求出的嵌段共聚物(B)的损耗角正切(tanδ)的峰值温度为-50℃以上-5℃以下。绘图:无;版权:(C)2017,JPO&INPI Ť

著录项

  • 公开/公告号JP2016210878A

    专利类型

  • 公开/公告日2016-12-15

    原文格式PDF

  • 申请/专利权人 ASAHI KASEI CORP;

    申请/专利号JP20150094896

  • 申请日2015-05-07

  • 分类号C08L95/00;C08L91/00;C08L53/02;C08F8/04;E01C7/18;

  • 国家 JP

  • 入库时间 2022-08-21 14:00:07

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号