BINDER FOR BOND MAGNET, COMPOSITION FOR BOND MAGNET, BOND MAGNET, AND METHOD FOR MANUFACTURING THE SAME

机译:用于粘结磁体的粘结剂,用于粘结磁体的组合物,粘结磁体及其制造方法

摘要

PROBLEM TO BE SOLVED: To provide a binder for a bond magnet having a long pot life.SOLUTION: The present invention relates to a binder for a bond magnet, which comprises: silsesquioxane expressed by [RSiO][RSiO][RSiO], and having a weight-average molecular weight of 2000 or less; and a siloxane compound having a hydrosilyl group, a hydrogen functional group chemical equivalent of 50-300 g/mol, and a weight-average molecular weight of 2000 or less, where Rrepresents a styryl group or an alkenyl group with 2-20C, Rrepresents an alkyl group with 1-20C, an aryl group with 6-20C, or an aralkyl group with 7-20C, Rrepresents an alkyl group with 1-10C, a styryl group, or an alkenyl group with 2-20C, l is a number of 0.05 to 0.9, m is a number of 0 to 0.85, and n is a number of 0.1 to 0.95, and l+m+n=1.SELECTED DRAWING: None
机译:解决的问题:提供一种适用期长的粘结磁体用粘合剂。解决方案:本发明涉及粘结磁体用粘合剂,其包含:以[RSiO] [RSiO] [RSiO]表示的倍半硅氧烷。重均分子量为2000以下; R 1为具有2至20C的苯乙烯基或烯基,且具有氢硅烷基,氢官能团化学当量为50〜300g / mol,重均分子量为2000以下的硅氧烷化合物。 R表示具有1-20C的烷基,具有6-20C的芳基或具有7-20C的芳烷基,R表示具有1-20C的烷基,苯乙烯基或烯基,具有2-20C。 0.05到0.9的整数,m是0到0.85的整数,n是0.1到0.95的整数,并且l + m + n = 1。

著录项

  • 公开/公告号JP2017112164A

    专利类型

  • 公开/公告日2017-06-22

    原文格式PDF

  • 申请/专利权人 3M INNOVATIVE PROPERTIES CO;

    申请/专利号JP20150243884

  • 发明设计人 HIROSHIGE YUJI;JITENDRA S RATHORE;

    申请日2015-12-15

  • 分类号H01F1/08;H01F1/113;H01F41/02;C08L83/07;C08L83/05;C08K3;C08G77/20;

  • 国家 JP

  • 入库时间 2022-08-21 13:59:16

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号