Solid photocatalyst material comprising solid material composed only of titanium dioxide having photocatalytic function, and method for producing the same
Solid photocatalyst material comprising solid material composed only of titanium dioxide having photocatalytic function, and method for producing the same
展开▼
机译:包括仅由具有光催化功能的二氧化钛组成的固体材料的固体光催化剂材料及其制造方法
展开▼
页面导航
摘要
著录项
相似文献
摘要
Provided are a solid photocatalyst material comprising a solid material (no carrier) composed only of titanium dioxide having a photocatalytic function, and a method for producing the same. The present invention consists of a solid material composed only of titanium dioxide of anatase type crystal (may include brookite type crystal) without containing a rutile type crystal, and the following i) to vi); i) fine Pore distribution 5 nm to 15 nm, ii) specific surface area 70 to 110 m 2 / g, iii) true density 3.90 ± 1.0 g / cm 3, iv) bulk specific gravity 1.3 to 1.6, v) Vickers hardness Is a solid photocatalyst material satisfying each numerical value of 600 to 800 Hv, vi) crystal grain size of 50 to 80 nm, and a method for producing the same. [Effect] A new material that does not require the addition of a carrier composed of solid titanium dioxide composed of only the same anatase type crystal (may include brookite type crystal) from the outer shell to the inner core of the solid. Provide a solid photocatalyst material of the type. [Selection] Figure 6
展开▼
机译:提供一种固体光催化剂材料及其制造方法,该固体光催化剂材料包括仅由具有光催化功能的二氧化钛构成的固体材料(无载体)。本发明由仅由锐钛矿型晶体的二氧化钛(可能包括板钛矿型晶体)组成,而不含金红石型晶体,以及以下i)至vi)的固体材料组成; i)细孔分布5 nm至15 nm,ii)比表面积70至110 m 2 / g,iii)真密度3.90±1.0 g / cm 3,iv)体积比重1.3至1.6,v)维氏硬度为分别满足600〜800Hv的数值,vi)50〜80nm的结晶粒径的固体光催化剂材料及其制造方法。 [效果]一种新材料,不需要从固体的外壳到内芯添加由仅由相同的锐钛矿型晶体(可能包括板钛矿型晶体)组成的固体二氧化钛构成的载体。提供这种类型的固体光催化剂材料。 [选择]图6
展开▼