首页> 外国专利> Insulating resin composition for DC power cable, resin cross-linked body, DC power cable, reinforcing insulation layer forming member for DC power cable connecting part and DC power cable connecting part

Insulating resin composition for DC power cable, resin cross-linked body, DC power cable, reinforcing insulation layer forming member for DC power cable connecting part and DC power cable connecting part

机译:直流电力电缆用绝缘树脂组合物,树脂交联体,直流电力电缆,直流电力电缆连接部和直流电力电缆连接部的加强绝缘层形成部件

摘要

[PROBLEMS] To form an insulating layer that has excellent extrudability, is resistant to sag, has good scorch resistance, has a small amount of secondary cracked water, and stably exhibits good direct current electric characteristics. To provide an insulating resin composition for a DC power cable having excellent properties. (A) Complex viscosity η * 100 at 130 ° C. and frequency 100 rad / s is 600 to 1300 Pa · s, complex viscosity η * 0.1 at 130 ° C. and frequency 0.1 rad / s, and complex viscosity η * From a mixture of low density polyethylene having a ratio (η * 0.1 / η * 100) of 100 or more, (B) modified polyethylene, (C) hindered phenol antioxidant and thioether antioxidant The amount of the carbonyl group introduced into the resin composition by the component (B) relative to the total mass of the component (A), the component (B) and the component (C) 7 × 10 −6 to 1.3 × 10 −5 mol / g. [Selection] Figure 1
机译:[问题]形成具有优异的可挤出性,耐流挂性,耐焦烧性,二次裂化水量少并且稳定地表现出良好的直流电特性的绝缘层。提供具有优异性能的用于DC电力电缆的绝缘树脂组合物。 (A)在130°C和100 rad / s的频率下的复数粘度η* 100为600至1300 Pa·s,在130°C和0.1 rad / s的频率下的复数粘度η* 0.1,以及复数η*从(η* 0.1 /η* 100)比为100或更高的低密度聚乙烯的混合物,(B)改性聚乙烯,(C)受阻酚抗氧化剂和硫醚抗氧化剂。相对于(A)成分,(B)成分和(C)成分的总质量,(B)成分为7×10 -6〜1.3×10 -5 mol / g。 [选择]图1

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号