首页> 外国专利> METHOD FOR PRODUCING A TUBULAR SEMIFINISHED PRODUCT FROM QUARTZ GLASS, METHOD FOR PRODUCING AN OPTICAL COMPONENT USING THE SEMIFINISHED PRODUCT, AND SEMIFINISHED PRODUCT CONSISTING OF QUARTZ GLASS DOPED WITH FLUORINE

METHOD FOR PRODUCING A TUBULAR SEMIFINISHED PRODUCT FROM QUARTZ GLASS, METHOD FOR PRODUCING AN OPTICAL COMPONENT USING THE SEMIFINISHED PRODUCT, AND SEMIFINISHED PRODUCT CONSISTING OF QUARTZ GLASS DOPED WITH FLUORINE

机译:由石英玻璃制备管状半成品的方法,使用该半成品制备光学组分的方法以及由掺有氟的石英玻璃制成的半成品

摘要

The aim of the invention is to improve a generally known method for producing quartz glass doped with fluorine, wherein SiO2 particles are formed in the presence of fluorine by means of a plasma deposition process, deposited in layers on an outer envelope of a cylindrical quartz glass substrate body rotating about its longitudinal axis, and vitrified to form a layer of quartz glass with a fluorine content of at least 1.5 wt. %, in such a way that a quartz glass semifinished product with a high fluorine content, characterised by a high basic transmission in the UV wavelength range, is obtained. To this end, the substrate body has at least one reservoir layer of quartz glass at least in the region of the outer envelope thereof, having a minimum hydroxyl group content of 200 wt. ppm and/or a minimum hydrogen content of 1×1017 molecules/cm3, and the substrate body is either fully or partially removed following the deposition of the quartz glass layer doped with fluorine.
机译:发明内容本发明的目的是改进用于制造掺有氟的石英玻璃的通常已知的方法,其中在存在氟的情况下通过等离子沉积工艺在SiO 2上沉积SiO 2 <Sub 2 颗粒。圆柱形石英玻璃基板主体的外壳,其围绕其纵轴旋转,并玻璃化形成一层氟含量至少为1.5 wt%的石英玻璃。 %,以这样的方式获得具有高氟含量的石英玻璃半成品,其特征在于在UV波长范围内的高基本透射率。为此,基体至少在其外壳的区域中具有至少一个石英玻璃储存层,其最小羟基含量为200wt。%。 ppm和/或最低氢含量为1×10 17 molesules / cm 3 ,并且在沉积石英玻璃层之后完全或部分去除了基体掺氟。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利