The present invention relates to a method for constructing a continuously reinforced concrete pavement using foam shotcrete by: positioning continuous reinforcement bars on a base layer where a concrete pavement is constructed; producing normal concrete having a compressive strength of 21-30 MPa from a batch plant and transporting same to a construction site; and shooting a normal strength concrete, which has been produced by mixing, with a mixing part, fly ash or fine slag powder or a low-grade mixed material produced by mixing the fly and the fine slag powder in a state in which fluidity has been increased by mixing in 20-40% of air bubbles with respect to volume, or shooting a high-performance concrete, which has been produced by mixing, with the mixing part, one or a mixture of two or more of silica fume, meta-kaolin, latex, polymers, and a coloring material.
机译:本发明涉及一种使用泡沫喷射混凝土建造连续增强混凝土路面的方法,该方法是:将连续增强杆放置在构造混凝土路面的基础层上;从分批工厂生产抗压强度为21-30 MPa的普通混凝土,并将其运输到施工现场;喷射普通强度混凝土,该普通强度混凝土通过将粉煤灰或炉渣细粉或通过将粉煤灰和炉渣细粉在流动性已混合的状态下混合而制得的低等级混合材料与混合部分混合而制得通过将20-40%的气泡(相对于体积)进行混合,或喷射一种高性能混凝土(通过将一种或两种或多种硅粉,一种或多种硅粉的混合物与混合部分混合而制成)来提高高岭土,乳胶,聚合物和着色材料。

著录项

  • 公开/公告号US2016333533A1

    专利类型

  • 公开/公告日2016-11-17

    原文格式PDF

  • 申请/专利号US201515112354

  • 发明设计人 KYONG KU YUN;

    申请日2015-01-12

  • 分类号E01C11/18;E01C11/20;E01C19/22;C04B18/08;C04B14/06;C04B14/10;C04B16/04;C04B18/14;E01C7/14;C04B38/10;

  • 国家 US