Ceramic cathode material of solid oxide fuel cell and manufacturing method thereof
Ceramic cathode material of solid oxide fuel cell and manufacturing method thereof
展开▼
机译:固体氧化物燃料电池的陶瓷正极材料及其制造方法
展开▼
页面导航
摘要
著录项
相似文献
摘要
A ceramic cathode material of a solid oxide fuel cell and a manufacturing method thereof are disclosed. The method includes mixing a lanthanum-containing compound, a cobalt-containing compound, a nickel-containing compound, and a copper-containing compound, for preparing the ceramic cathode material of the solid oxide fuel cell of intermediate/low type. The ceramic cathode material of the solid oxide fuel cell is LaCozNiyCuxO3−δ, in which x ranges from 0.01 to 0.3, y ranges from 0 to 0.89, and z ranges from 0.1 to 0.99. The ceramic cathode material manufactured by mixing the lanthanum-containing compound, the cobalt-containing compound, the nickel-containing compound, and the copper-containing compound when operating within the temperature range from 500 to 800 degrees Celsius is of high electrical conductivity and reduced thermal expansion coefficient.
展开▼
机译:公开了一种固体氧化物燃料电池的陶瓷阴极材料及其制造方法。该方法包括混合含镧化合物,含钴化合物,含镍化合物和含铜化合物,以制备中/低型固体氧化物燃料电池的陶瓷阴极材料。固体氧化物燃料电池的陶瓷阴极材料为LaCo z Sub> Ni y Sub> Cu x Sub> O 3-δ Sub>,其中x的范围是0.01到0.3,y的范围是0到0.89,z的范围是0.1到0.99。当在500至800摄氏度的温度范围内操作时,通过将含镧的化合物,含钴的化合物,含镍的化合物和含铜的化合物混合而制造的陶瓷阴极材料具有高电导率并降低了热膨胀系数。
展开▼