摘要

A method for preparing a homogeneous braid-reinforced (HMR) PPTA hollow fiber membrane combines PPTA hollow tubular braids with PPTA surface separation layer. The method includes following steps of: (1) preparing the PPTA hollow tubular braids, wherein the PPTA hollow tubular braids which are made from PPTA filament yarns are woven by a two-dimensional braided method, the outer diameter of the PPTA tubular braids is 1-2 mm; (2) preparing the PPTA casting solution as the surface separation layer, wherein the 1-3 wt % PPTA resin, 0-2 wt % inorganic particles and 10-20 wt % pore-forming agents are mixed into 75-89% inorganic acid solvent, stirred for 1-3 hours at 70° C.-90° C. to form homogeneous and transparent casting solution; and (3) preparing reinforced PPTA hollow fiber membrane, wherein the casting solution as the surface separation layer is evenly coated on the surfaces of the PPTA hollow tubular braids through spinneret, and they are immersed in a coagulation bath for solidified formation.
机译:一种制备均质编织增强(HMR)PPTA中空纤维膜的方法,其将PPTA中空管状编织物与PPTA表面分离层结合在一起。该方法包括以下步骤:(1)制备PPTA中空管状编织物,其中,由PPTA长丝纱线制成的PPTA中空管状编织物通过二维编织法编织而成,PPTA中空编织物的外径为1。 -2毫米; (2)制备PPTA浇铸溶液作为表面分离层,其中将1-3重量%的PPTA树脂,0-2重量%的无机颗粒和10-20重量%的成孔剂混合到75-89%的无机酸中。溶剂,在70°C-90°C下搅拌1-3小时,形成均匀透明的流延溶液; (3)制备增强的PPTA中空纤维膜,其中,作为表面分离层的流延溶液通过喷丝头均匀地涂覆在PPTA中空管状编织物的表面上,并浸入凝固浴中凝固。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号