patent specification: "polymerization or copolymerization process of unsaturated ethylene monomers in the presence of free radical polymerization initiators". polymerization or copolymerization process of ethylene unsaturated monomers in the presence of free radical polymerization initiators at pressures from 110 mpa to 500 mpa and at temperatures from 100 ° to 350 ° c in a continuously operated polymerization apparatus where the gas composition The reaction gas is compressed to polymerization pressure by at least two compressors in sequential operation where a low pressure compressor first compresses the reaction gas composition to a pressure ranging from 10 mpa to 50 mpa and where A high pressure compressor then compresses the reaction gas composition to the polymerization pressure where the high pressure compressor is operated with a polyalkylene glycol-based synthetic lubricant and oxygen is introduced into the fresh gas inlet or polymerization apparatus in an amount such that the composition of the gas to be compressed in the compressor High pressure gas has an oxygen content ranging from 0.01 ppm to 0.9 ppm and process for operating a compressor to pressurize unsaturated monomers with ethylene to a pressure of 5 mpa to 500 mpa where the compressor is lubricated with a lubricant polyalkylene glycol-based synthetic compound and where the composition of the gas to be pressurized has an oxygen content ranging from 0.01 ppm to 0.9 ppm. 21169235v1
机译:专利说明书:“在自由基聚合引发剂的存在下,不饱和乙烯单体的聚合或共聚方法”。在连续操作的聚合设备中,在自由基聚合引发剂的存在下,在自由基聚合引发剂的存在下,在压力为110 mpa至500 mpa且温度为100°至350°c的条件下,进行乙烯不饱和单体的聚合或共聚过程至少两个压缩机在顺序操作中的聚合压力,其中低压压缩机首先将反应气体组成压缩到10 mpa至50 mpa的压力,然后高压压缩机将反应气体组成压缩到聚合压力,在高压力下高压压缩机使用聚亚烷基二醇类合成润滑剂操作,将氧气引入新鲜气体入口或聚合设备,其加入量应使压缩机中被压缩的气体的组成高压气体的氧含量范围为0.01 ppm至0.9 ppm的操作流程用乙烯将不饱和单体加压至5 mpa至500 mpa的压气机,其中压气机用润滑剂聚亚烷基二醇基合成化合物润滑,并且被压气的成分的氧含量范围为0.01 ppm至0.9 ppm。 21169235v1

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号