Polyurethane adhesive comprises: a first component comprising (a) at least one triol with a molecular weight of 1000-10000 g/mole, (b) at least one diol with two primary hydroxyl groups and a molecular weight of 60-150 g/mole, and (c) at least one aliphatic polyamine having a molecular weight of 60-500 g/mole; a second component comprising (d) at least one polyisocyanate and (e) at least one isocyanate polyurethane polymer; and additional polyurethane adhesive comprising (f) at least one catalyst in the form of a metal chelate complex, in which metal is e.g. iron(III) and hafnium(IV). Polyurethane adhesive comprises: a first component comprising (a) at least one triol with a molecular weight of 1000-10000 g/mole, (b) at least one diol with two primary hydroxyl groups and a molecular weight of 60-150 g/mole, and (c) at least one aliphatic polyamine having a molecular weight of 60-500 g/mole; a second component comprising (d) at least one polyisocyanate and (e) at least one isocyanate polyurethane polymer; and additional polyurethane adhesive comprising (f) at least one catalyst in the form of a metal chelate complex, in which the metal is iron(III), titanium(IV), zirconium(IV) and hafnium(IV). The triol, diol and polyamine are present in an amount such that the ratio of the number of hydroxy groups and amino groups of (diol and polyamine) to triol is 3-15, and the ratio of the number of hydroxy groups and amino groups of diol to polyamine is 2-30. Independent claims are also included for: (1) bonding a first substrate to a second substrate, comprising mixing the two components of the polyurethane adhesive, applying the mixed polyurethane adhesive to at least one of the substrate surfaces to be bonded, joining the substrates to be bonded within the open time, and curing the polyurethane adhesive; and (2) an article produced from the above mentioned method.
机译:聚氨酯粘合剂包括:第一组分,其包含(a)至少一种分子量为1000-10000 g / mol的三醇,(b)至少一种具有两个伯羟基且分子量为60-150 g / mol的二醇(c)至少一种分子量为60-500 g / mol的脂族多胺;第二组分,其包含(d)至少一种多异氰酸酯和(e)至少一种异氰酸酯聚氨酯聚合物;以及另外的聚氨酯粘合剂,其包含(f)至少一种金属螯合物的形式的催化剂,其中金属是例如金属。铁(III)和ha(IV)。聚氨酯粘合剂包括:第一组分,其包含(a)至少一种分子量为1000-10000 g / mol的三醇,(b)至少一种具有两个伯羟基且分子量为60-150 g / mol的二醇(c)至少一种分子量为60-500 g / mol的脂族多胺;第二组分,其包含(d)至少一种多异氰酸酯和(e)至少一种异氰酸酯聚氨酯聚合物;以及另外的聚氨酯粘合剂,其包含(f)至少一种金属螯合物形式的催化剂,其中金属是铁(III),钛(IV),锆(IV)和ha(IV)。三醇,二醇和多胺的存在量使得(二醇和多胺)的羟基和氨基的数量与三醇的比例为3-15,并且三醇,二醇和多胺的羟基的数量与三醇的比例为3-15。二醇对多胺为2-30。还包括以下独立权利要求:(1)将第一基底粘合到第二基底,包括混合聚氨酯粘合剂的两种组分,将混合的聚氨酯粘合剂施涂到至少一个要粘合的基底表面上,将基底连接至在开放时间内粘合,并固化聚氨酯胶粘剂; (2)根据上述方法制造的物品。

著录项

  • 公开/公告号BR112015004214A2

    专利类型

  • 公开/公告日2017-08-08

    原文格式PDF

  • 申请/专利权人 SIKA TECHNOLOGY AG;

    申请/专利号BR20151104214

  • 发明设计人 RITA CANNAS;STEFFEN KELCH;URS BURCKHARDT;

    申请日2013-09-10

  • 分类号C08G18/32;C08G18/48;C08G18/66;C08G18/76;

  • 国家 BR

  • 入库时间 2022-08-21 13:40:17

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号