Aluminium alloy intended especially for manufacture of castings of mold segments for molding pneumatic tires and heat treatment process of mold segment castings

机译:专门用于制造用于模制充气轮胎的模具段铸件和模具段铸件的热处理工艺的铝合金

摘要

ufeffpu0159edmu011btnu00e1 aluminum alloy contains 85,55 when 89,00% by weight. al; 8.5 to 10% by weight. a; 0.6 to 1.2% by weight. cu; 0.6 to 1.0% by weight. ni; 0.4 to 0.8% by weight. mn, 0.03 to 0.05% by weight. sr; a maximum of 0.4% by weight. mg; maximum 0,6% by weight. fe; max 0,1% by weight. you; max 0,1% by weight. zn and max. 0,05% by weight. other ingredients individually, while the other additives total max is 0,15% by weight.the subject invention is method of heat treatment of castings segments forms of this alloy, which are those segments forms ohu0159u00e1ty on u017eu00edhacu00ed temperature 520 degrees and u017eu00edhu00e1ny for 0.5 to 8 h, then returned in the water at a temperature of 50 to 60 degrees celsius and then make out the by aging at a temperature of 170 degrees c for 6 to 8 hours.
机译:当重量为89,00%时,铝合金包含85,55。 al; 8.5至10重量%。一种; 0.6至1.2重量%。 cu; 0.6至1.0重量%。你; 0.4至0.8重量%。 mn,0.03至0.05重量%。 sr;最多0.4%(重量)。毫克;最高0.6%重量。 ;最高0.1%重量。您;最高0.1%重量。 zn和max。 0,05重量%。其他成分单独添加,而其他添加剂的总和最大为0.15%(重量)。本发明是该合金铸件链段形式的热处理方法,这些链段形式为 u017e u00edhac 在520度的温度下放置0.5到8小时,然后在50到60摄氏度的温度下放回水中,然后在170摄氏度的温度下老化6到8个小时。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号