The present invention provides a method for steam curing of steel making slag including reduction of free alkaline earth oxide with volume expansion less than 2% by injecting steam in a vessel charged with slag under variable conditions of pressure and temperature in shorter time compared to prior Arts. The slag is crushed and ground to a size of 6-80 mm and is charged into the apparatus (V) at normal temperature through a conveyor belt (8). The half top of the vessel (V) is closed tight enough to maintain the pressure substantially higher than atmosphere. Steam is passed via a moisture separator (10) to the vessel (V) through a nozzle arrangement disposed in the middle of a disc type arrangement provided at the bottom of the vessel when the interior of the apparatus (V) is maintained under a pressure of 2.5 --3.5 Kg/cm2 for a period of 24 to 72 years at a bed height of 2m. of steel making slag. The hot condensate is taken out continuously as a neutralising agent and the pressure of the vessel is made equal to atmospheric pressure when the slag is discharged from the vessel (V) and collected in storage tank (11).
机译:本发明提供了一种用于炼钢炉渣的蒸汽固化的方法,该方法包括通过在比现有技术短的时间内在压力和温度的可变条件下向装有炉渣的容器中注入蒸汽,以减少体积膨胀小于2%的方式还原游离碱土金属氧化物。 。将炉渣压碎并研磨成6-80 mm的大小,然后在常温下通过传送带(8)装入设备(V)。容器(V)的半顶部密封得足够紧,以保持压力大大高于大气压。当装置(V)的内部保持在压力下时,蒸汽通过水分分离器(10)通过设置在容器底部的圆盘式装置中间的喷嘴装置进入容器(V)。 2.5 --3.5 Kg / cm2,床高2m时为24至72年。炼钢渣。当炉渣从容器(V)中排出并收集到储罐(11)中时,连续取出热的冷凝液作为中和剂,并使容器的压力等于大气压。

著录项

相似文献

  • 专利
  • 外文文献
  • 中文文献
获取专利

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号